Your Professional Nickel Alloy Coil Strip Foil Manufacturer

 

Lork Group specializes in supplying nickel alloy coil, strip foil stock. Common materials include Hastelloy, Monel, Inconel, Incoloy, Haynes, and Nimonic, among others. Our stock complies with ASTM, AISI, AMS, JIS, GB, and other relevant standards. This coil strip foil stock is commonly used in aerospace, medical, and industrial applications. We stock coil strip foil in sizes ranging from Thickness: 0.02mm - 16.0mm, Width: 5mm - 3000mm, with custom lengths available. Most importantly, we support third-party testing and have extensive customer experience verifying our pipe and tube stock

  • Monel 404 Alloy Strip (ASTM F96 / W.Nr. 2.4867)

    Monel 404 tape is a precision material used to create the crucial metal-glass interface in electronic devices. As long as the iron content is precisely controlled, the annealing process is correctly

  • Alloy 42 Nickel Strip (UNS K94100 /ASTM F30)

    Alloy 42 is a nickel-iron alloy (approximately 42% nickel and 58% iron). Its core value lies not in its strength or corrosion resistance, but in its coefficient of thermal expansion, which closely

  • Hastelloy Alloy C2000 Strip (UNS N06200 / W.Nr. 2.4675 / ...

    Hastelloy C2000 is a nickel-based alloy designed to withstand a variety of harsh corrosive environments. ASTM B575 is a common standard for Hastelloy C2000 nickel alloy strips.

  • Nimonic 75 Nickel Alloy Strip

    Nimonic 75 nickel alloy strip generally complies with standards such as GB/T 2072 (Nickel and Nickel Alloy Strip), AMS 5758 (Aerospace Material Specification), ASTM B536 (UNS N06075), and DIN 17752.

  • ASTM B409 Haynes HR120 Nickel Alloy

    Haynes HR-120 is a solid solution strengthened nickel-iron alloy. It offers high temperature resistance, high strength, and excellent resistance to carburization and sulfidation environments. It is

  • ASTM B575 Hastelloy C-4 Nickel Alloy Strip

    Hastelloy C-4 nickel alloy strip is commonly used in flue gas desulfurization (FGD) systems. The commonly used standard for strip is ASTM B575. Lork Group's general ASTM B575 Hastelloy C-4 Nickel

  • UNS 09902 Ni-Span-C Alloy 902 Nickel Strip

    Ni-Span-C Alloy 902 is a precipitation-hardenable nickel-iron alloy with constant elasticity as its key characteristic. We typically supply UNS 09902 Ni-Span-C Alloy 902 Nickel Strip, delivered in

  • Monel 401 Strip

    Monel 401 (UNS N04401) is a nickel-copper alloy with a very low coefficient of electrical resistivity and resistance to a wide variety of corrosive conditions. Like with commercially pure Nickel,

  • Hastelloy B3 Nickel Alloy Strip (ASTM B333,UNS N010675)

    Lork Group is a reliable manufacturer and supplier of Hastelloy B3 strip and coil in China. It's a high performance nickel molybdenum alloy. It has excellent resistance to reduction.

  • Hastelloy C276 Nickel Strip

    Hastelloy C276 is a highly representative nickel-based alloy, renowned for its excellent overall corrosion resistance, especially in harsh chemical environments. Strip is a very important product

  • Hastelloy C22 Strip

    Lork Group is a reliable manufacturer and supplier of Hastelloy C22 strip and coil in China. Hastelloy C22 alloy (UNS N06022) is a nickel-chromium-molybdenum alloy materials.

  • Haynes 188 Strip

    Haynes 188 strip is not age hardenable, but may be cold worked to achieve higher tensile and yield strength. Alloy 188 is non-magnetic. It performs well in continuous high temperature service and

First 12 Last

 

Custom Nickel Alloy Coil Strip Foil

We provide custom nickel alloy coil strip foil manufacturing solutions to meet your project needs. Customizable Options:

1. Material Type:

We have a variety of nickel alloy types to choose from.

 

2. size:

Thickness: 0.02mm - 16.0mm, Width: 5mm - 3000mm, Customizable upon request.

 

3. Surface Treatment:

We offer galvanizing, aluminizing, oxidation, and other surface treatment processes, which can be customized to meet your specific requirements upon request.

 

4. Flatness and curl:

Customizable upon request.

Haynes 188 Strip

 

Our Best-Selling Nickel Alloy Coil Strip Foil

 

Monel 401 Strip

Monel 401 (UNS N04401) is a nickel-copper alloy with a very low coefficient of electrical resistivity and resistance to a wide variety of corrosive conditions. Like with commercially pure Nickel, Alloy 401 is low in strength in the annealed condition and can only be cold worked to a maximum of 120 KSI.

 

Hastelloy B3 Strip

Lork Group is a reliable manufacturer and supplier of Hastelloy B3 strip and coil in China. It's a high-performance nickel molybdenum alloy. It has excellent resistance to reduction.

 

Hastelloy C276 Strip

Lork Group is a reliable manufacturer and supplier of Hastelloy C276 strip and coil in China. The alloy is resistant to pitting, crevice corrosion, and stress corrosion cracking.

 

Monel K500 Strip

Monel K500 strip is a precipitation-strengthening alloy. It consists of nickel, copper, and aluminum. This alloy has extremely high strength and corrosion resistance.

 

Nickel Alloy Coil Strip Foil Chemical Composition

 

Element

Content (%)

Nickel, Ni

40 – 45 max

Copper, Cu

Remainder

Manganese, Mn

2.25 max

Iron, Fe

0.75 max

Silicon, Si

0.25 max

Cobalt, Co

0.25 max

Carbon, C

0.10 max

Sulfur, S

0.015 max

 

Nickel Alloy Coil Strip Foil Physical Properties

 

Density

g/cm³

9.22

lb/in.³

0.333

Modulus Of Elasticity (E)

At 70°F (20°C)

31.4 x 10³ ksi (216 GPa)

Modulus Of Rigidity (G)

At 70°F (20°C)

12.0 x 10³ ksi (83 GPa)

Electrical Resistivity

53.8 µΩ.in, (137 µΩ.cm)

Thermal Conductivity

78.0 Btu-in/ft2hr-°F, (11.2 W/m-K)

Coefficient Of Expansion

6.6 µin/in.-°F (70°F to 1000°F)

11.8 µm/m-°C (20°C to 538°C)

 

Nickel Alloy Coil Strip Foil Mechanical Properties

 

Annealed

Heat Treatment

2050°F (1121°C)

Tensile Strength

120 – 160 ksi (830 – 1100 MPa)

Suggested Operating Conditions

-300°F to 750°F (-184°C to 400°C)

Spring Temper

Tensile Strength

200 – 240 ksi (1380 – 1655 MPa)

Suggested Operating Conditions

-300°F to 750°F (-184°C to 400°C)

 

Nickel Alloy Coil Strip Foil Material

 

nickel alloy & cobalt alloy

Inconel

Hastelloy

Monel

Incoloy

Inconel 625

Inconel 718

Inconel 600

Inconel X750

Inconel 601

Inconel 617

Inconel 690

Inconel 738LC

Inconel 713C

Inconel 602CA

Inconel 725

Inconel 686

Inconel 751

Hastelloy C276

Hastelloy C22

Hastelloy X

Hastelloy C4

Hastelloy B2

Hastelloy G30

Hastelloy C2000

Hastelloy B3

Hastelloy G

Hastelloy N

Hastelloy S

Hastelloy W

Hastelloy G3

Monel 400

Monel k500

Monel r405

Monel 404

Monel 401

Monel 450

Incoloy 800

Incoloy 825

Incoloy 925

Incoloy 800ht

Incoloy 909

Incoloy 901

Incoloy 840

Incoloy 20

Incoloy 28

Incoloy 330

Incoloy 907

Incoloy 945

Incoloy 903

Incoloy A286

Haynes Alloy

Nimonic Alloy

Other Alloy

Haynes 230

Haynes 282

Haynes 188

Haynes 214

Haynes 556

Haynes 242

Haynes 25

Haynes 233

Haynes 244

Haynes 263

Nimonic 90

Nimonic 80a

Nimonic 75

Nimonic 115

Nimonic 901

Nimonic 105

Nimonic 263

Alloy 42

Alloy 45

Invar 42

Invar 36

Kovar

Maraging 250

Maraging 300

Maraging 350

MP159

Rene 41

Waspaloy

MP35N

 

Quality Inspection Procedures

productcate-1-1
Spectrometer
productcate-1-1
Ultrasonic Testing
productcate-1-1
Stress Corrosion Testing
productcate-1-1
Microcopy
productcate-1-1
Mechanical
productcate-1-1
Eddy Current Test
productcate-1-1
Heat Treatment Furnace
productcate-1-1
Corrosion Test
productcate-1-1
Hydraulic Test
productcate-1-1
Metallographic Test

FAQ

Q: How is the nickel alloy Coil Strip Foil manufactured?

A: It is typically produced through processes like hot rolling, cold rolling, and annealing. A correct chemical composition is necessary to give uniform and required properties to different alloys. The alloys are then melted, Hot-Rolled, and processed to final sizes using state-of-the-art technology.

Q: What are the mechanical properties of the nickel alloy strip?

A: Mechanical properties include tensile strength, yield strength, and hardness.

Q: How does the nickel content affect the properties of the alloy strip?

A: Higher nickel content often leads to better corrosion resistance and heat resistance.

Q: Can a nickel alloy strip be welded?

A: Although the weldability of nickel and its alloys is generally good, the composition, metallurgical structure, and its heat treatment and/or service history all affect its response to welding. Wrought, fine-grained components have better weldability than cast items, as these often have significant amounts of segregation.

Q: How strong is the ickel alloy strip?

A: These are characterised by their high resistance to corrosion at both normal and high temperatures (resistance to scaling), good high-temperature strength, and high electrical resistance.

We're well-known as one of the leading nickel alloy strip manufacturers in China. Please feel free to buy cheap nickel alloy strip for sale here and get pricelist from our factory. For price consultation, contact us.

Send Inquiry