Hastelloy B-3 Nickel Alloy Strip (UNS N010675)
Lork Group is a reliable manufacturer and supplier of Hastelloy B3 strip and coil in China. Hastelloy B3 (UNS N10675) is a high performance nickel molybdenum alloy. It has excellent resistance to reduction. As a premium solid solution strengthened alloy, has very high strength.
We produce Hastelloy B3 strip according to ASTM B333 by default. Due to the very high strength of Hastelloy B3, its deformation during cold rolling is smaller than that of other alloys. Therefore Hastelloy B3 strip requires more cold rolling passes than other alloys. This made the production very difficult. Many suppliers cannot guarantee the quality of the finished product. We put a lot of effort into producing this alloy. Ultimately, we were able to deliver the Hastelloy B3 strip perfectly.
As a leading Hastelloy alloy strip and coil supplier in China, Lork Group manufactures and produces Hastelloy B3 strip of various sizes. If you have any mechanical requirements, please confirm with we. We can customize the material exactly to your requirements.
Chemical Composition
|
Element |
% |
|
C |
0.01 max |
|
Mn |
3.00 max |
|
Si |
0.10 max |
|
P |
0.030 max |
|
S |
0.010 max |
|
Cr |
1.00 – 3.00 |
|
Co |
3.00 max |
|
Mo |
27.00 – 32.00 |
|
V |
0.20 max |
|
Fe |
1.00 – 3.00 |
|
Al |
0.50 max |
|
W |
3.00 max |
|
Ni |
65.00 min |
Physical Properties
|
Density |
g/cm³ |
9.22 |
|
lb/in.³ |
0.333 |
|
|
Modulus of Elasticity (E) |
At 70°F (20°C) |
31.4 x 10³ ksi (216 GPa) |
|
Modulus of Rigidity (G) |
At 70°F (20°C) |
12.0 x 10³ ksi (83 GPa) |
|
Electrical Resistivity |
53.8 µΩ.in, (137 µΩ.cm) |
|
|
Thermal Conductivity |
78.0 Btu-in/ft2hr-°F, (11.2 W/m-K) |
|
|
Coefficient of Expansion |
6.6 µin/in.-°F (70°F to 1000°F) |
|
|
11.8 µm/m-°C (20°C to 538°C) |
||
Mechanical Properties
|
Annealed |
Heat Treatment |
2100°F (1150°C) |
|
Tensile Strength |
110 ksi (760 MPa) min 125 ksi (860 MPa) typ |
|
|
Suggested Operating Conditions |
-300°F to 1800°F (-184°C to 900°C) |
Application
- Chemical processing
- Vacuum furnaces
- Mechanical components
Hot Tags: ASTM B333 strip,UNS N010675 strip,Alloy B-3 strip,Hastelloy B-3 Nickel Alloy Strip,Hastelloy B-3 strip Supplier