UNS 09902 Ni-Span-C Alloy 902 Nickel Strip

UNS 09902 Ni-Span-C Alloy 902 Nickel Strip

Ni-Span-C Alloy 902 is a precipitation-hardenable nickel-iron alloy with constant elasticity as its key characteristic. We typically supply UNS 09902 Ni-Span-C Alloy 902 Nickel Strip, delivered in either solution or cold-rolled condition. For technical data sheets, please contact us!
Send Inquiry

 

UNS 09902 Ni-Span-C Alloy 902 Nickel Strip Description

 

Ni-Span-C Alloy 902 (also known as UNS N09902) is a unique precipitation-hardening nickel-iron-chromium alloy. Its most notable features are its ability to maintain a nearly constant elastic modulus over a wide temperature range (approximately -45°C to +65°C or -50°C to +150°C) and an extremely low coefficient of thermal expansion.

 

Lork Group supplies UNS 09902 Ni-Span-C Alloy 902 Nickel Strip, typically in thicknesses of 0.04mm to 5.0mm (or as thin as 0.025mm/0.03mm). Please click the circle icon below to initiate an online communication.

 

 

UNS 09902 Ni-Span-C Alloy 902 Nickel Strip Parameters

 

 

 

 Ni-Span-C Alloy 902 Custom

Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft nickel alloys for you!.
UNS 09902 Ni-Span-C Alloy 902

Ni-Span-C Alloy 902 Bar

Specifications

UNS N09902
ASTM F15
UNS 09902 Ni-Span-C Alloy 902 plate

Ni-Span-C Alloy 902 Plate

Specifications

UNS N09902
3J53
UNS 09902 Ni-Span-C 902 Nickel Alloy Strip

Ni-Span-C Alloy 902 Strip

Specifications

UNS N09902
ASTM F15
Ni-Span-C Alloy 902

Ni-Span-C Alloy 902 Strip

Specifications

AMS 5221
AMS 5223
AMS 5225

 

Ni-Span-C Alloy 902 Nickel Strip Manufacturing and Pricing Reference

 

 

Ni-Span-C Alloy 902 Nickel Strip

   Aging:

    Aging treatment (e.g., 650°C for 4 hours) is essential after forming and is a key step in achieving strengthening and constant elastic properties.

   Stress Relief:

   After cold working, a low-temperature (e.g., 400°C) stress relief annealing helps reduce deformation during subsequent aging, which is particularly important for thin strips.

     Lork Group offers customized UNS 09902 Ni-Span-C Alloy 902 Nickel Strip. Approximate prices are as follows:
1. Stock Material: $25-30/kg (MOQ 30kg), $20/kg (100kg)
2. Custom Material - SAE AMS 5221 (solution annealed), AMS 5223 (10% cold rolled), AMS 5225 (50% cold rolled)(Price based on your requirements)
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

Ni-Span-C Alloy 902 Nickel Strip

 

 The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information! 

 

 

Ni-Span-C Alloy 902 Chemical Composition

 

 

Weight% Ni-Span-C Alloy 902
Ni 41.0 - 43.5%
Cr 4.90 - 5.75%
Ai 0.30 - 0.80%
Ti 2.20 - 2.75%
Fe Bal

 

 

Ni-Span-C Alloy 902 Mechanical Properties

 

 

Material Ni-Span-C Alloy 902
Tensile Strength 1210 MPa
Shear Modulus 62-69 GPa
Elastic Modulus 165-200 GPa

 

For more UNS 09902 Ni-Span-C Alloy 902 Nickel Strip details, please contact us!

 

Contact now

Hot Tags: uns 09902 ni-span-c alloy 902 nickel strip, China uns 09902 ni-span-c alloy 902 nickel strip manufacturers, factory