Lork Group specializes in supplying pipe and tube stock in five materials: nickel alloy, cobalt alloy, titanium alloy, precision alloy, and stainless steel. We maintain inventory standards in accordance with ASTM, AISI, AMS, JIS, GB, and other relevant standards. This pipe stock is commonly used in aerospace, medical, and industrial applications. We stock tubes in sizes ranging from Outside diameter: 6mm - 1219mm, Thickness: 0.5mm - 100mm, (Capillary Pipe: Outside diameter: 0.5mm - 6.0 mm, Thickness: 0.05mm - 2.0mm) with custom lengths available. Most importantly, we support third-party testing and have extensive customer experience verifying our pipe and tube stock, ensuring peace of mind in your selection and reliable delivery!

  • 17-4 PH Pipe

    17-4 PH pipe is a martensitic precipitation hardening stainless steel with additions of copper (Cu), niobium (Nb) and tantalum (Ta). The grade combines high strength and hardness values with moderate

  • AMS 5581 Inconel 625 Nickel Alloy

    Its core competitive advantage lies in the combination of niobium solid-solution strengthening and molybdenum corrosion resistance. It is easy to weld and suitable for use across a wide temperature

  • HyMu 80 Permalloy Alloy Tube

    HyMu 80 permalloy tubes require strict control over nickel content (80%), molybdenum content (4-5%), proper final annealing (1177℃ dry hydrogen), and a magnetic performance report (μi≥20000) to be

  • 310moLN Stainless Steel Pipe (UNS S31050 / ASTM A213)

    310MoLN stainless steel pipe is a triple insurance against deformation, corrosion, and carburization in complex flue gas environments at extreme high temperatures (up to 1150°C). It is a battle armor

  • Ni-Span C Alloy 902 (ASTM F30, UNS K94610)

    Ni-Span C is a nickel-iron-chromium constant elasticity alloy. Its core value lies in the fact that its elastic modulus (Young's modulus E) changes very little within a certain temperature range

  • Permalloy 80 Pipe (ASTM A753,Ni80)

    Permalloy is a type of nickel-iron soft magnetic alloy with extremely high permeability and extremely low coercivity. It is a magnetic highway that is extremely sensitive to external magnetic fields.

  • Incoloy 926 Nickel Alloy Pipe (UNS N08926,DIN 25-6Mo,W.Nr...

    Incoloy 926 (also known as Alloy 926) is not a general-purpose material. It is a high-end austenitic alloy specifically developed to address extremely harsh halide (especially chloride) corrosion

  • Inconel 725 Nickel Alloy Pipe(ASTM B805,UNS N07725)

    Lork Group supplies Inconel 725, a high-performance nickel-chromium-molybdenum alloy that resists stress corrosion cracking in deep and ultra-deep oil and gas extraction operations. As long as the

  • Hastelloy C2000 Nickel Alloy Capillary Tube

    Common range: OD 6-530mm, wall 0.5-50mm, length 1-12m per ASTM B622. Delivery condition: solution annealed. Specify tolerances clearly.

  • Nickel 200 Alloy Capillary Tube

    Delivery condition matters: soft (annealed/M state), semi-hard, or hard state. Affects processing and final performance. Choose wisely.

  • UNS S32760 Duplex Pipe

    UNS S32760 duplex pipe is a super duplex stainless steel with a microstructure of 50% austenite and 50% ferrite. has very good resistance to localized corrosion and stress corrosion cracking in

  • Hastelloy C276 Pipe

    Hastelloy C276 Pipe is a Nickel-chromium-molybdenum wrought alloy, resistant to pitting and crevice corrosion attacks. The addition of tungsten to the composition of the makes it one of the most

First 12345 Last

Custom Pipe And Tube 

 

We provide custom pipe and tube manufacturing solutions to meet your project needs. Customizable Options:

1. Material Type:

We provide different types of materials to choose from.

 

2. Size:

Can be customized upon request.

 

3. Shape:

Can be customized upon request.

 

4. Surface Treatment:

We provide polishing, painting, electroplating and other surface treatment processes, which can be customized upon request.

 

5. Color

Can be customized upon request.

Incoloy 864 Alloy Pipe

 

Types of Pipe And Tube

 

 

Nickel Alloy Pipe

Nickel alloy pipes are a type of steel pipe made from a combination of nickel and other elements, such as chromium, molybdenum, iron, copper, and titanium.

 

Stainless Steel Tube

Stainless steel tubes are hollow, cylindrical structures used both as components in machinery and as conduits for fluid transport.

 

Pipe And Tube Specification

 

Type

Cold Drawn / Welded / ERW

Outer Diameter Size

Seamless - 1/4" NB to 6" NB (Nominal Bore Size)
Welded / ERW- 1" NB to 16" NB (Nominal Bore Size)

Wall Thickness

Schedule 10 to Schedule 160

Length

5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.

Ends

Plain Ends / Beveled Ends

Delivery Conditions

As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered

Coating

Electropolish, Mechanical Polish, Satin Finish, Passivated

Other Testing

NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc.

Dimension

All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME

Value Added Services

Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment

 

Pipe And Tube Chemical Composition

 

Element

Content (%)

Iron, Fe

73

Chromium, Cr

15.0 - 17.5

Nickel, Ni

3.0 - 5.0

Copper, Cu

3.0 - 5.0

Manganese, Mn

1.0

Silicon, Si

1.0

Tantalum, Ta

0.45

Niobium, Nb (Columbium, Cb)

0.45

Nb + Ta

0.15 - 0.45

Carbon, C

0.070

Phosphorous, P

0.040

Sulfur, S

0.030

 

Pipe And Tube Mechanical Properties

 

Properties

Metric

Imperial

Tensile Strength

730-930 MPa

105877 - 134885 psi

Proof Strength

530 MPa

76870 psi

Modulus Of Elasticity

200 GPa

29007 ksi

Elongation At Break (In 50 Mm)

25%

25%

 

Pipe And Tube Thermal Properties

 

Properties

Metric

Imperial

Thermal expansion co-efficient (@100°C/212°F)

14.7 µm/m°C

8.17 µin/in°F

Thermal conductivity (@23°C/73.4°F)

11 W/mK

76.3 BTU.in/hrft².°F

 

Pipe And Tube Stock Material

 

Spot Sale

 

Pipe And Tube Outside Dimension Tolerances

 

Largest Outside Dim.

Gauge Range

+/- Tolerance

.625

20ga - 14ga

.004"

Over .625" - 1.125" inc.

20ga - 11ga

.005"

Over 1.125" - 1.5" inc.

20ga - 10ga

.006"

Over 1.5" - 2" inc.

16ga - 7ga

.008"

Over 2" - 3" inc.

16ga - 7ga

.01"

Pipe And Tube Surface Treatment

 

productcate-1-1

 

Application of Pipe And Tube

 

● Construction industry

 

● Oil and gas industry

 

● Shipbuilding industry

 

● Textile industry

 

● Agricultural industry

 

● Industrial applications

 

● Additional applications

AISI 316 316L Pipe

 

AISI 321 Pipe

● Power plants

 

● Diary and food processing facilities

 

● Modern architecture

 

● Chemical facilities

 

● Water treatment facilities

 

● Synthetic fiber production

 

● Desalination

 

● Energy industries

 Quality Inspection Procedures

productcate-1-1
Spectrometer
productcate-1-1
Ultrasonic Testing
productcate-1-1
Stress Corrosion Testing
productcate-1-1
Microcopy
productcate-1-1
Mechanical
productcate-1-1
Eddy Current Test
productcate-1-1
Heat Treatment Furnace
productcate-1-1
Corrosion Test
productcate-1-1
Hydraulic Test
productcate-1-1
Metallographic Test

FAQ

Q: What can pipes and tubes be used for?

A: Since pipe and tube is both durable and lightweight, it's commonly utilized by the construction industry in commercial and residential buildings, as well as in industry sectors including power, water, sewer, manufacturing and more.

Q: What is your minimum order quantity?

A: Our minimum order quantity is 50 kg. Larger quantity, lower price.

Q: What is the advantage of pipe and tube?

A: Using stainless pipe and tubes gives you a durable product that will last for decades. Steel is a reliable material that is easy to maintain and install. Stainless steel is very low-maintenance, and because of its corrosion-resistant properties, it's unlikely it will need to be replaced for decades.

Q: How do you control product quality?

A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.

Q: Can you provide processing services?

A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.

Q: Can you provide samples?

A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.

We're well-known as one of the leading pipe and tube manufacturers in China. Please feel free to buy cheap pipe and tube for sale here and get pricelist from our factory. For price consultation, contact us.

Send Inquiry