• 17-7 PH Strip

    17-7 PH Strip is a precipitation hardening stainless steel strip that provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum

  • 17-4 PH Strip

    17-4 PH Strip also called EN 1.4542 precipitation hardening stainless steel strip.The strength, toughness, ductility and weldability of it are comparable to those of grade 304 stainless steel strips.

  • PH 15-7mo Stainless Steel Strip

    PH 15-7mo Stainless Steel Strip is a semi-austenitic precipitation hardening strip that provides high strength and hardness, good corrosion resistance, and minimum distortion upon heat treatment.

  • AL6XN Strip

    AL-6XN Strip also has resistance to a wide range of other corrosive environments, including protection from chloride induced stress corrosion cracking and pitting/crevice corrosion in oxidizing

  • 254 SMO Alloy Strip

    Lork Group is a reliable Chinese manufacturer and supplier of 254 SMO alloy strips and coils. This alloy demonstrates outstanding resistance to pitting, crevice corrosion, stress cracking, and

  • 2507 Duplex Stainless Steel Strip

    2507 Duplex Stainless Steel Strip has excellent resistance to stress corrosion cracking as well as pitting, crevice, and erosion corrosion. Alloy 2507 also has high thermal conductivity, a low

  • 2205 Duplex Stainless Steel Strip

    Lork Group is a reliable manufacturer and supplier of 2205 Duplex Stainless Steel Strip and Coil in China. Type 2205 is a duplex (austenitic/ferritic) stainless steel alloyed with chromium,

  • Hastelloy B3 Nickel Alloy Strip (ASTM B333,UNS N010675)

    Lork Group is a reliable manufacturer and supplier of Hastelloy B3 strip and coil in China. It's a high performance nickel molybdenum alloy. It has excellent resistance to reduction.

  • Hastelloy C276 Nickel Strip

    Hastelloy C276 is a highly representative nickel-based alloy, renowned for its excellent overall corrosion resistance, especially in harsh chemical environments. Strip is a very important product

  • Hastelloy C22 Strip

    Lork Group is a reliable manufacturer and supplier of Hastelloy C22 strip and coil in China. Hastelloy C22 alloy (UNS N06022) is a nickel-chromium-molybdenum alloy materials.

  • Haynes 188 Strip

    Haynes 188 strip is not age hardenable, but may be cold worked to achieve higher tensile and yield strength. Alloy 188 is non-magnetic. It performs well in continuous high temperature service and

  • Incoloy 825 Strip

    Incoloy 825 strip is ductile over a wide range of temperatures from cryogenic to well in excess of 1000 °F (538 °C). Fabricability is typical for a nickel alloy, with the material readily formable