2507 Duplex Stainless Steel Strip

2507 Duplex Stainless Steel Strip

2507 Duplex Stainless Steel Strip has excellent resistance to stress corrosion cracking as well as pitting, crevice, and erosion corrosion. Alloy 2507 also has high thermal conductivity, a low coefficient of thermal expansion, and good weldability.
Send Inquiry

Type 2507 is a super-duplex (austenitic/ferritic) stainless steel designed for applications that require exceptional strength and corrosion resistance surpassing that of 304 and 316 stainless steels.

 

2507 Duplex Stainless Steel Strip has excellent resistance to stress corrosion cracking as well as pitting, crevice, and erosion corrosion. Alloy 2507 also has high thermal conductivity, a low coefficient of thermal expansion, and good weldability.

 

The material is supplied in a solution-annealed state, with a thickness ranging from 0.015 mm to 3.5 mm and a maximum width of 300 mm. It is available in 2B, BA, and surface treatments to meet various processing requirements such as stamping, deep drawing, and welding.

 

Chemical Composition

 

Element

%

C

0.030 max

Mn

1.20 max

Si

0.80 max

P

0.035 max

S

0.020 max

Cr

24.0 – 26.0

Ni

6.0 – 8.0

Mo

3.0 – 5.0

N

0.24 – 0.32

Cu

0.50 max

 

Physical Properties

 

Density

g/cm³

7.8

lb/in.³

0.280

Modulus of Elasticity (E)

At 70°F (20°C)

29.0 x 10³ ksi (200 GPa)

Modulus of Rigidity (G)

At 70°F (20°C)

10.9 x 10³ ksi (75 GPa)

Electrical Resistivity

32.7 µohm-in, (83.0 µohm-cm)

Thermal Conductivity

118 Btu-in/ft2hr-°F
17.0 W/m-°C

Coefficient of Expansion

7.2 µin/in.-°F (70-212°F)

12.96 µm/m-°C (20-100°C)

 

Mechanical Properties

Annealed

Heat Treatment

1920-2100°F (1050-1150°C)

Tensile Strength

1150-145 ksi (800-1000 MPa)

Suggested Operating Conditions

-58°F to 572°F (-50°C to 300°C)

 

 

Processing available

 

Slitting/Cutting, Leveling/Length Cutting

Cold-rolled strip surface treatment: 2B, BA, No.1, and other surface finishes

 

Welding consumables: ER2594 (welding wire) or E2594 (welding electrode) are recommended for welding, and interpass temperature control is necessary.

 

 

Advanced manufacturing processes

 

Optimize hot rolling process

 

01

Edge crack control

Utilizing an optimized hot rolling process, edge crack depth is controlled to within 5mm, resulting in a high yield.

Solution annealing

 

02

σ phase suppression

Precise solution annealing followed by water quenching effectively suppresses σ-phase precipitation and ensures equilibrium of the biphase microstructure.

Suitable for harsh environments

 

03

Purity control

Ultra-low inclusion control ensures corrosion resistance, making it suitable for harsh working conditions, such as those found in seawater and chemical industries.

Supporting services

 

04

Supporting services

We provide slitting, leveling, and length processing services, as well as the selection of matching welding materials.

 

 

Surface Treatment

 

product-1200-750

 

 

Lork Group
Marketing Operations Department
 Email: layla@lorkgroup.com
 WhatsApp: +86 199 3707 5488

 

Hot Tags: 2507 duplex stainless steel strip,2507 duplex stainless steel strip manufacturers, 2507 Duplex Stainless Steel, ASTM A240/A240M, UNS S32750

Send Inquiry