PH 15-7Mo Stainless Steel Strip (UNS S15700)
Lork Group is a reliable manufacturer and supplier of PH 15-7mo Stainless Steel Strip and Coil in China. Grade PH 15-7 Mo strip, also known as UNS S15700 strip. It comes from the chemical compositions of chromium (15.0%), nickel (7.0%), molybdenum (2.0%), and aluminum (1.10%).
It is a semi-austenitic precipitation hardening strip that provides high strength and hardness, good corrosion resistance, and minimum distortion upon heat treatment.
PH 15-7 Mo exhibits better corrosion resistance than 17-4 PH stainless steel strip in most environments. PH 15-7 Mo is magnetic in both the annealed and hardened conditions.
PH 15-7 Mo material is used for parts requiring high strength, moderate corrosion resistance where a combination of high mechanical strength with good ductility is required after heat treatment.
As a leading Stainless Steel strip and coil supplier in China, Lork Group manufactures and produces PH 15-7mo Stainless Steel Strip of various sizes. If you have any mechanical requirements, please confirm with we. We can customize the material exactly to your requirements.
Chemical Composition
|
Element |
% |
|
C |
0.09 |
|
Mn |
1.00 |
|
Si |
1.00 |
|
P |
0.04 |
|
S |
0.03 |
|
Cr |
14-16 |
|
Ni |
6.50-7.75 |
|
Mo |
2-3 |
|
AI |
0.75-1.5 |
Mechanical Properties
|
Grade |
Condition |
Thickness (inch) |
Tensile Strength (ksi) |
Yield Strength (ksi) |
Elongation % |
Hardness |
|
PH 15-7 Mo/UNS S15700 |
Solution Treated |
<0.005 |
150 (max) |
65 (max) |
25 |
100 HB (max) |
|
PH 15-7 Mo/UNS S15700 |
TH1050 (AMS 5520) |
0.010-0.020 |
190 |
170 |
4 |
40 HRC |
|
PH 15-7 Mo/UNS S15700 |
TH1050 (AMS 5520) |
0.020-0.1875 |
190 |
170 |
5 |
40 HRC |
|
PH 15-7 Mo/UNS S15700 |
TH1050 (AMS 5520) |
0.1875-0.500 |
190 |
170 |
6 |
40 HRC |
|
PH 15-7 Mo/UNS S15700 |
RH950 (AMS 5520) |
0.010-0.020 |
225 |
220 |
3 |
45 HRC |
|
PH 15-7 Mo/UNS S15700 |
RH950 (AMS 5520) |
0.020-0.1875 |
225 |
220 |
4 |
45 HRC |
|
PH 15-7 Mo/UNS S15700 |
RH950 (AMS 5520) |
0.1875-0.500 |
225 |
220 |
5 |
45 HRC |
|
PH 15-7 Mo/UNS S15700 |
Condition C |
– |
200 |
175 |
1 |
41 HRC |
|
PH 15-7 Mo/UNS S15700 |
Condition CH900 |
– |
240 |
230 |
1 |
46 HRC |
Application
PH 15-7 Mo stainless steel strip has excellent corrosion resistance and mechanical properties, making it an ideal material for many different industries. The most common applications include:
- Aircraft structural parts
- Aircraft interior parts
- Aerospace components
- Medical instruments and implants
- Food processing equipment
- Food handling conveyor belts and chains
- Jewelry and watches
Hot Tags: PH 15-7Mo, 15-7PH, Stainless Steel Strip, UNS S15700, semi-austenitic stainless steel, precipitation hardening strip, high strength strip, spring strip, aircraft strip