2205 Duplex Stainless Steel Strip (UNS S32205)

2205 Duplex Stainless Steel Strip (UNS S32205)

Lork Group is a reliable manufacturer and supplier of 2205 Duplex Stainless Steel Strip and Coil in China. Type 2205 is a duplex (austenitic/ferritic) stainless steel alloyed with chromium, molybdenum, and nitrogen for improved performance and corrosion resistance compared to 304 and 316 stainless steels.
Send Inquiry

Lork Group is a reliable manufacturer and supplier of 2205 Duplex Stainless Steel Strip and Coil in China. Type 2205 is a duplex (austenitic/ferritic) stainless steel alloyed with chromium, molybdenum, and nitrogen for improved performance and corrosion resistance compared to 304 and 316 stainless steels.

 

Features of 2205 Duplex Stainless Steel Strip

 

Corrosion Resistance: The 2205 stainless steel bar offers excellent corrosion resistance, making it ideal for use in harsh environments. It effectively resists corrosion from a wide range of chemicals, including acids, alkalis, and chlorides.

High Strength: With high strength, 2205 stainless steel strip is perfect for applications requiring robust mechanical strength. Its yield strength reaches up to 450 MPa, and its tensile strength can go up to 620 MPa.

Duplex Structure: The duplex structure of 2205 stainless steel strip provides exceptional resistance to stress corrosion cracking, pitting, and crevice corrosion. Additionally, it boasts good weldability and formability.

Heat Resistance: 2205 stainless steel strip exhibits good heat resistance, making it suitable for high-temperature applications. It can withstand temperatures up to 300°C.

As a leading Duplex Stainless Steel strip and coil supplier in China, Lork Group manufactures and produces 2205 Duplex Stainless Steel Strip of various sizes. If you have any mechanical requirements, please confirm with we. We can customize the material exactly to your requirements.

 

Chemical Composition

 

Element

%

C

0.03 max

Mn

2.00 max

Si

1.00 max

P

0.03 max

S

0.02 max

Cr

22.0 – 23.0

Ni

4.5 – 6.5

Mo

3 – 3.5

Fe

Balance

N

0.14 – 0.20

 

Physical Properties

 

Density

g/cm³

7.86

lb/in.³

0.284

Modulus of Elasticity (E)

At 70°F (20°C)

29.0 x 10³ ksi (200 GPa)

Electrical Resistivity

33.5 µohm-in, (85.1 µohm-cm)

Thermal Conductivity

104 Btu-in/ft2-hr-°F
15.0 W/m-°C

Coefficient of Expansion

11.1 µin/in.-°F (70-2000°F)

14.0 µm/m-°C (0-300°C)

 

Mechanical Properties

 

Annealed

Heat Treatment

1868-2050°F (1020-1121°C)

Tensile Strength

120 – 150 ksi (825-1035 MPa)

Suggested Operating Conditions

-58°F to 572°F (-50 to 300°C)

Spring Temper

Heat Treatment

Stress relieve as needed

Tensile Strength

200 ksi (1300 MPa)

Suggested Operating Conditions

Up to 550°F (288°C)

 

Application

 

  • Mixing tanks
  • Heat exchangers
  • Pressure vessels
  • Extraction/distillation columns
  • Pulp processing equipment
  • Pipes
  • Pumps
  • Food processing equipment
  • Springs

 

Surface Treatment

 

product-1200-750

 

 

Hot Tags: 2205 Duplex, Duplex 2205, Stainless Steel Strip, UNS S32205, Ferritic-Austenitic Steel, High Strength Strip, Chloride Resistant Strip