15-5PH Stainless Steel Pipe
Introduction to 15-5ph stainless steel Pipe
Steel 15-5 is a variant of the older 17-4 and 15-5 was designed to have greater toughness than S17400, especially in the through-thickness (short transverse) direction. Alloy 15-5 is used in applications that require high transverse strength and toughness such as engine parts, aircraft components, nuclear reactor components etc.
We keep a selection of common sizes of 15-5PH stainless steel pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us request a quote.
Specification
15-5 VM COND H-1050 to the following specifications
AMS-5659 T-1 (EXC. COND)
AMS-H-6875
ASTM-A-484
ASTM-A-564 TYPE XM-12 (EXC. COND)
BAC-5619 (150-170 MIN. TENS.)
AMS 5862 Sheet, Strip and Plate.
AMS 5826 Welding Wire
UNS : S15500
15-5PH Powder - ASTM A564

15-5PH stainless steel Chemical Composition
|
Element |
Content (%) |
|
Iron, Fe |
75 |
|
Chromium, Cr |
14.48 |
|
Nickel, Ni |
4.5 |
|
Copper, Cu |
3.5 |
|
Manganese, Mn |
≤1 |
|
Silicon, Si |
≤1 |
|
Nb + Ta |
0.3 |
15-5PH Pipe Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile Strength |
1380 MPa |
200000 psi |
|
Yield Strength |
1275 MPa |
184900 psi |
|
Modulus of Elasticity |
200 GPa |
29000 ksi |
|
Elongation at Break |
10% |
10% |
|
Hardness, Brinell |
420 |
420 |
|
Hardness, Knoop |
451 |
451 |
|
Hardness, Rockwell B |
104 |
104 |
|
Hardness, Rockewell C |
44.2 |
44.2 |
|
Hardness, Vickers |
445 |
445 |
|
Charpy Impact |
10 J |
7.38 ft.lb |
15-5PH stainless steel pipe Application
- Marine gas turbine compressor sections
- Hallow shafts
- Paper mill equipment
- Engine parts
- Aircraft components
- Gears