17-4 PH Stainless Steel Pipe (UNS S17400)
Lork Group is a leading supplier and exporter of 17-4 PH pipes and tubes. 17-4 PH is a martensitic precipitation-hardening stainless steel with additions of copper (Cu), niobium (Nb), and tantalum (Ta). The grade combines high strength and hardness values with moderate corrosion resistance. Different heat treatment temperatures can optimize mechanical properties, e.g., yield strength at 1100 – 1300MPa.
17-4PH pipe has good fabricating characteristics and can be age-hardened by a single-step, low-temperature treatment. Is a versatile material widely used in the aerospace, chemical, petrochemical, food processing, paper, and general metalworking industries.
Characteristics
- High strength
- Hardness (up to 572°F /300°C)
- Corrosion resistance
- Mechanical properties can be optimized with heat treatment.
- Very high yield strength up to 1100-1300 MPa (160-190 ksi) can be achieved.
We keep a selection of common sizes of 17-4 PH pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us and request a quote. susan@lorkgroup.com | +86 199 3707 5488
Specification
|
Type |
Cold Drawn / Welded / ERW |
|
Outer Diameter Size |
Seamless - 1/4" NB to 6" NB (Nominal Bore Size) |
|
Wall Thickness |
Schedule 10 to Schedule 160 |
|
Length |
5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
|
Ends |
Plain Ends / Beveled Ends |
|
Delivery Conditions |
As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
|
Coating |
Electropolish, Mechanical Polish, Satin Finish, Passivated |
|
Other Testing |
NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current Test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved, etc. |
|
Dimension |
All pipes are manufactured and Inspected / Tested to the Relevant standards, including ASTM and ASME |
|
Value Added Services |
Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
|
Packaging |
Loose / Bundle / Wooden Pallet / Wooden box / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
Chemical Composition
|
Element |
Content (%) |
|
Iron, Fe |
73 |
|
Chromium, Cr |
15.0 - 17.5 |
|
Nickel, Ni |
3.0 - 5.0 |
|
Copper, Cu |
3.0 - 5.0 |
|
Manganese, Mn |
1.0 |
|
Silicon, Si |
1.0 |
|
Tantalum, Ta |
0.45 |
|
Niobium, Nb (Columbium, Cb) |
0.45 |
|
Nb + Ta |
0.15 - 0.45 |
|
Carbon, C |
0.070 |
|
Phosphorus, P |
0.040 |
|
Sulfur, S |
0.030 |
Physical Properties
|
Properties |
Metric |
Imperial |
|
Density |
7.75 g/cm3 |
0.280 lb/in³ |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Shear modulus |
77.4 GPa |
11200 ksi |
|
Elastic modulus |
190-210 GPa |
27557-30458 ksi |
|
Poisson's ratio |
0.27-0.30 |
0.27-0.30 |
|
Hardness, Brinell |
352 |
352 |
|
Hardness, Knoop (estimated from Rockwell C) |
363 |
363 |
|
Hardness, Rockwell C |
36 |
36 |
|
Hardness, Vickers (estimated from Rockwell C) |
349 |
349 |
Application
- Aerospace - structural and parts
- Biomedical - hand tools
- Chemical Processing
- Food Process Equipment
- Gate Valves
- Mechanical Components
- Nuclear Waste Processing and Storage
- Oil and Gas Production - foils, helicopter deck platforms, etc.
- Pulp and Paper - paper mill equipment
Hot Tags: 17-4PH Pipe, 17-4 PH Stainless Steel Pipe, UNS S17400, precipitation hardening stainless steel pipe, martensitic stainless pipe, seamless pipe, welded pipe