AISI 310 310S Stainless Steel Pipe (UNS S31000 S31008)

AISI 310 310S Stainless Steel Pipe (UNS S31000 S31008)

AISI 310/310S pipe high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation and the retention of a larger fraction of room temperature strength than the common austenitic alloys like Type 304.
Send Inquiry

Lork Group is a leading supplier and exporter of AISI 310/310S pipes and tubes. Stainless steel 310/310S is an austenitic heat-resistant alloy with excellent resistance to oxidation under mildly cyclic conditions up to 2000°F.

 

AISI 310/310S pipe's high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room-temperature strength than the common austenitic alloys like Type 304. Stainless 310 is often used at cryogenic temperatures, with excellent toughness to -450°F and low magnetic permeability.

 

Characteristics

 

  • Oxidation resistance to 2000°F
  • Moderate strength at high temperature
  • Resistance to hot corrosion
  • Strength and toughness at cryogenic temperatures

 

We keep a selection of common sizes of AISI 310/310S pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us and request a quote.

 

Specification

 

Type

Cold Drawn / Welded / ERW

Outer Diameter Size

Seamless - 1/4" NB to 6" NB (Nominal Bore Size)
Welded / ERW- 1" NB to 16" NB (Nominal Bore Size)

Wall Thickness

Schedule 10 to Schedule 160

Length

5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.

Ends

Plain Ends / Beveled Ends

Delivery Conditions

As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered

Coating

Electropolish, Mechanical Polish, Satin Finish, Passivated

Other Testing

NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current Test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved, etc.

Dimension

All pipes are manufactured and Inspected / Tested to the Relevant standards, including ASTM and ASME.

Value Added Services

Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment

Packaging

Loose / Bundle / Wooden Pallet / Wooden box / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector

 

Chemical Composition

 

Grade

C

Mn

Si

P

S

Cr

Mo

Ni

Fe

AISI 310

0.015 max

2.0 max

0.15 max

0.020 max

0.015 max

24.00 - 26.00

0.10 max

19.00 - 21.00

54.7 min

AISI 310S

0.08 max

2.0 max

1.00 max

0.045 max

0.030 max

24.00 - 26.00

0.75 max

19.00 - 21.00

53.095 min

 

Mechanical Properties

 

Density

Melting Point

Tensile Strength

Yield Strength (0.2%Offset)

Elongation

7.9 g/cm3

1402 °C (2555 °F)

Psi – 75000 , MPa – 515

Psi – 30000 , MPa – 205

40 %

 

Application

 

  • Kilns
  • Heat Exchangers
  • Radiant Tubes
  • Muffles, retorts, annealing covers
  • Tube hangers for petroleum refining and steam boilers
  • Coal gasifier internal components
  • Saggers
  • Furnace parts, conveyor belts, rollers, oven linings, fans
  • Food processing equipment
  • Cryogenic structures

 

 

Hot Tags: 310 Stainless Steel Pipe, 310S Stainless Steel Pipe, high-temperature pipe, oxidation-resistant pipe, austenitic stainless pipe, seamless pipe, welded pipe

Send Inquiry