PH 15-7mo Pipe
PH 15-7MO is a semi-austenitic precipitation-hardening stainless steel known for its outstanding mechanical properties. Key advantages include:
High Strength & Hardness – Ideal for structural components requiring superior load-bearing capacity.
- Excellent Corrosion Resistance – Performs well in harsh environments, including chemical and marine applications.
- Minimal Distortion After Heat Treatment – Ensures dimensional stability, reducing post-treatment machining needs.
- Formability in Annealed Condition – Easy to shape and fabricate before final hardening.
For extreme applications where maximum strength is critical, PH 15-7MO pipe in Condition CH 900 offers exceptional hardness with limited ductility, making it perfect for high-stress, high-temperature scenarios.
As a leading supplier and exporter, Lork Group specializes in providing top-quality PH 15-7MO pipes and tubes, ensuring reliability for critical applications across aerospace, chemical processing, and high-temperature environments
Specification
|
Type |
Cold Drawn / Welded / ERW |
|
Outer Diameter Size |
Seamless - 1/4" NB to 6" NB (Nominal Bore Size) |
|
Wall Thickness |
Schedule 10 to Schedule 160 |
|
Length |
5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length, and Customized Size. |
|
Ends |
Plain Ends / Beveled Ends |
|
Delivery Conditions |
As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
|
Coating |
Electropolish, Mechanical Polish, Satin Finish, Passivated |
|
Other Testing |
NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved, etc. |
|
Dimension |
All Pipes are manufactured and inspected/tested to the Relevant standards, including ASTM and ASME |
|
Value Added Services |
Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
|
Packaging |
Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
Chemical Composition
|
Element |
Content (%) |
|
Iron, Fe |
Balance |
|
Chromium, Cr |
14 -16 |
|
Nickel, Ni |
6.50 - 7.75 |
|
Molybdenum, Mb |
2 - 3 |
|
Silicon, Si |
1 |
|
Manganese, Mn |
1 |
|
Aluminum, Al |
0.75 - 1.50 |
|
Carbon, C |
0.09 |
|
Phosphorus, P |
0.040 |
|
Sulfur, S |
0.040 |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile Strength |
650 - 880 MPa |
94275 - 127633 psi |
|
Yield Strength |
350 - 550 MPa |
50763 - 79771 psi |
|
Elongation at Break |
8 - 25% |
10% |
|
Young's Modulus |
200 GPa |
29008 ksi |
Application
- Paneling and springs
- Diaphragms
- Retaining rings
- Welded and brazed honeycomb paneling
- Aircraft components bulkheads
Stock Availability & Fast Delivery
At Lork Group, we maintain a ready inventory of PH 15-7MO pipes in common sizes to meet urgent project demands. Whether you need standard dimensions or custom specifications, our team ensures timely delivery without compromising quality.
If your project requires high-strength PH 15-7MO pipe with fast turnaround times, contact Lork Group for competitive pricing and expert support. Let us provide the stainless steel solution that meets your toughest engineering challenges.
Optimize performance-choose PH 15-7MO pipe from a trusted global supplier!
Surface Treatment

Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.
Hot Tags: ph 15-7mo pipe, China ph 15-7mo pipe manufacturers, factory
You Might Also Like
Send Inquiry