Nimonic 80A Nickel Alloy Bar
Nimonic 80A nickel bar is a forgeable, age-hardenable nickel-chromium alloy. 80A alloy manufactured by Lork Group has good corrosion and oxidation resistance while maintaining high tensile strength
-
Nimonic 105 Nickel Alloy Bar
Nimonic 105 is a nickel-cobalt-chromium-based precipitation-hardening wrought superalloy, renowned for its exceptional strength, creep resistance, and oxidation resistance at high temperatures. It
-
Haynes 214 Nickel Alloy Strip
Haynes 214 is a nickel-chromium-aluminum-iron alloy designed for high-temperature environments, typically 955°C (1750°F) and above. It offers excellent oxidation resistance. Haynes 214 nickel alloy
-
Inconel 718 Nickel Alloy Mold
Inconel 718 is a nickel alloy with unparalleled strength, stability, and durability under extreme environments (high temperature, high pressure, strong corrosion). If your mold working conditions are
-
Haynes HR160 Nickel Alloy Bar
Haynes HR160 is a solid solution strengthened nickel-based superalloy designed to maintain excellent stability in extremely high-temperature and corrosive environments. This type of material is
-
Haynes HR120 Nickel Alloy Bar
Haynes HR120 is a solid solution strengthened iron-nickel-chromium-based superalloy. Its key properties include excellent high-temperature strength (up to 1095°C), good resistance to carburization
-
Nickel 200 Nickel Alloy Strip
Nickel 200 is a solid solution-reinforced material made of commercially pure nickel (nickel content ≥99.0%). Its core value lies in its superior corrosion resistance to alkaline environments,
-
Haynes 282 Nickel Alloy Strip
Haynes 282 is an alloy designed for cutting-edge applications that demand extreme high-temperature strength without compromising manufacturability. The key to sourcing it lies in selecting reliable
-
Monel R405 Nickel Alloy Plate
As a purchasing professional, understanding Monel R405 alloy steel plate hinges on its outstanding advantages in easy machinability and resistance to chloride ion corrosion.
-
Haynes 617 Nickel Alloy Plate
Haynes 617 (also often called Inconel 617) is a top-grade high-temperature alloy plate, a material used in high-pressure situations, and must be purchased with utmost care.
-
Nimonic 90 Nickel Alloy Sheet
Nimonic 90 Alloy Sheet is a Nickel-Chromium-Cobalt alloy being precipitation hardenable, strengthened by the addition of Titanium and Aluminium.
-
AMS 5544 Waspaloy Alloy Sheet
AMS 5544 Waspaloy Alloy Sheet is a nickel based age hardenable alloy that possesses high temperature strength while still having a good corrosion resistance, especially to oxidation.