• ASTM B168 Inconel 693 Nickel Alloy

    Inconel 693 is a high-nickel-chromium alloy that is resistant to high-temperature corrosion, with high-temperature oxidation resistance being key. Lork Group typically supplies ASTM B168 Inconel 693

  • Haynes 617 Nickel Alloy(ASTM B166)

    Haynes 617 is an excellent nickel-chromium-cobalt-molybdenum-aluminum-titanium system solid solution strengthened high-temperature alloy, known for its excellent high-temperature strength, oxidation

  • Haynes 242 Nickel Alloy(UNS N10242)

    Lork Group Haynes 242 alloy is produced in the form of reforge billet, bar, plate, sheet, and wire welding products, all in various sizes. Get premium quality, fast delivery, and request a free

  • Monel 400 Copper Nickel Alloy Sheet

    Monel 400 Plate is a copper-nickel alloy made metallic plate. Monel 400 Plate has good ductility and corrosion resistance to a variety of corrosive media.

  • Hastelloy S Nickel Alloy(UNS N06635)

    Hastelloy S is a nickel-cobalt-molybdenum high-temperature alloy with excellent thermal stability, oxidation resistance and low thermal expansion. Lork Group supplies Hastelloy S nickel alloy in

  • Nimonic 75 Nickel Alloy (UNS N06075)

    Nimonic 75 is a nickel-chromium alloy with excellent corrosion and heat resistance. Lork offers Nimonic 75 nickel alloy in stock in various specifications, making it ideal for gas turbine engines,

  • AMS 5581 / Inconel 625 Seamless Tube

    Our manufactured sizing capabilities for Inconel 625 seamless tube and pipe ranges from 2-1/16” to 10-3/4” OD with wall thicknesses up to 1.925”. Please reach out for more information on our minimum

  • Inconel 690 Nickel Alloy (UNS N06690)

    Inconel 690 is a high-chromium nickel alloy characterized by corrosion resistance, high strength, good metallurgical stability, and excellent workability. It is commonly used in petrochemical

  • 2.4660 / UNS N08020 / Nickel Alloy 20

    Nickel Alloy 20 (UNS N08020 / 2.4660) is the optimal choice for sulfuric acid, chloride, and mixed acid environments. Its superior corrosion resistance, weldability, and mechanical strength make it

  • Hastelloy B-2 Nickel Plate(ASTM B575)

    Lork Group is a trusted global exporter and supplier of Hastelloy B-2 (UNS N10665 / 2.4617), the specialized nickel-molybdenum alloy renowned for its exceptional resistance to the most severe

  • UNS N0645 / Hastelloy C4 Nickel Sheet

    Hastelloy C-4 was designed to address the most critical drawback of Hastelloy C-276: thermal stability. The composition of C-4 has been specifically optimized so that, even without post-weld solution

  • Haynes HR160 Nickel Alloy(W.Nr.2.4880)

    Haynes HR160 has strong resistance to sulfidation in both oxidizing and reducing atmospheres, making it an ideal material for manufacturing waste incinerators. The W.Nr.2.4880 Haynes HR 160 Nickel