Haynes 214 Nickel Alloy Strip

Haynes 214 Nickel Alloy Strip

Haynes 214 is a nickel-chromium-aluminum-iron alloy designed for high-temperature environments, typically 955°C (1750°F) and above. It offers excellent oxidation resistance. Haynes 214 nickel alloy strip supplied by Lork Group is best suited for high-temperature, low-stress environments and is widely used in the aerospace, automotive, industrial heating, and medical industries.
Send Inquiry

Welcome to Lork Group, your specialty metals manufacturer and exporter.

 

Lork Group is a professional Haynes 214 nickel alloy strip exporter headquartered in China. Founded in 2010, after 15 years of development, the company has become one of the leaders in Chinese metal materials. We have more than 3,000 tons of permanent inventory. Lork Group stocks and processes hastelloy, monel,incoloy, inconel bars, plates, tubes, strip, foil, wire and other products.

If you are interested in Haynes 214 nickel alloy strip, please click the circle icon below to communicate online.

 

Nickel Alloy Haynes 214 parameters

 

 Haynes 214 Nickel Alloy stock
Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft nickel alloys for you!.
haynes 214 alloy bar
Nickel Alloy Bar
Specifications
UNS N07214
W.NR 2.4646
haynes 214 alloy sheet
Nickel Alloy Plate
Specifications
UNS N07214
AWS 061
haynes 214 alloy tube
Nickel Alloy Pipe
Specifications
UNS N07214
ASTM B366
haynes 214 alloy wire
Nickel Alloy Wire
Specifications
UNS N07214
W.NR 2.4646

 

Haynes 214 Strip Manufacturing Process and Challenges

    Recommended working and heat treatment parameters:

           Hot working: 1200-980 °C

           Soft annealing: 1065-1120 °C

    Hot working procedure - during the heat-up, if the piece hast both large and small cross-sections, equilibrate it at about 870°C. The best overall results seem to be achieved by working from a furnace temperature near 1150°C. Stop the operation when the piece reaches 980°C. Perform soft annealing.

    Alloy 214 can be cold worked, though subsequent soft annealing is required. Cold working promotes high-temperature ductility.

    Lork Group offers customized nickel alloy strip products in a variety of specifications for applications in aerospace, medical, oil and gas, and other fields. We have successful client collaborations.
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

haynes 214 strip

 

What are the common problems with Haynes 214?

Contact us, and we will reply to you!

Lork Haynes 25 wire
 

What is Haynes Alloy 214 strip?

The cutting surfaces on a vertical end mill bit (are for milling ) are on its sides , designed for cutting horizontally , a drill bit ( are for drilling ) cutting surface is at its tip , designed for cutting vertically downward .. you'll notice a end mill usually has a flat on the end of the bit .

 

What are the main characteristics of Haynes Alloy 214 Strip?

The cutting surfaces on a vertical end mill bit (are for milling ) are on its sides , designed for cutting horizontally , a drill bit ( are for drilling ) cutting surface is at its tip , designed for cutting vertically downward .. you'll notice a end mill usually has a flat on the end of the bit .

 

What industries is Haynes Alloy 214 wire typically used in?

The cutting surfaces on a vertical end mill bit (are for milling ) are on its sides , designed for cutting horizontally , a drill bit ( are for drilling ) cutting surface is at its tip , designed for cutting vertically downward .. you'll notice a end mill usually has a flat on the end of the bit .

 

How does Haynes 214 strip comply with industry standards?

The cutting surfaces on a vertical end mill bit (are for milling ) are on its sides , designed for cutting horizontally , a drill bit ( are for drilling ) cutting surface is at its tip , designed for cutting vertically downward .. you'll notice a end mill usually has a flat on the end of the bit .

Strip form characteristics:

 Haynes 214 strip is typically supplied in the solution heat-treated condition.

 It can be cold-rolled to various tempers and hardened by cold working or aging.

 Available in different finishes, including cold-rolled and precision-slit.

 Commonly supplied in coils or cut-to-length.

 