AISI 316 316L Pipe
Lork Group is a leading supplier and exporter of the AISI 316/316L pipe and tubes. Stainless Steel Pipe 316/316L is a tubular shaped 316/316L Stainless Steel Alloy pipe.
316 Stainless Steel is a standard molybdenum-bearing grade, the second most commonly sought after grade next to grade 304 amongst the austenitic stainless steels.
The molybdenum gives 316 better overall corrosion resistant properties than Grade 304, particularly higher resistance in chloride environments.
Grade 316L (L= low carbon) ) is the same as 316 except it has an extra-low-carbon analysis, the advantage of which is that it precludes any harmful precipitation in the 800º F to 1500º F range that might result from welding heavier sections. Therefore 316L is extensively used in heavy gauge welded components.
Typically there is no price difference between 316 and 316L stainless steel.
We keep a selection of common sizes of AISI 316/316L pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us request a quote.
Specification
|
Type |
Cold Drawn / Welded / ERW |
|
Outer Diameter Size |
Seamless - 1/4" NB to 6" NB (Nominal Bore Size) |
|
Wall Thickness |
Schedule 10 to Schedule 160 |
|
Length |
5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
|
Ends |
Plain Ends / Beveled Ends |
|
Delivery Conditions |
As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
|
Coating |
Electropolish, Mechanical Polish, Satin Finish, Passivated |
|
Other Testing |
NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc. |
|
Dimension |
All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME |
|
Value Added Services |
Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
|
Packaging |
Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
Chemical Composition
|
Element |
AISI 316 |
AISI 316L |
|
Carbon |
≤0.08 |
≤0.03 |
|
Manganese |
≤2.00 |
≤2.00 |
|
Phosphorus |
≤0.045 |
≤0.045 |
|
Sulfur |
≤0.030 |
≤0.030 |
|
Silicon |
≤0.75 |
≤0.75 |
|
Chromium |
16.00-18.00 |
16.00-18.00 |
|
Nickel |
10.00-14.00 |
10.00-14.00 |
|
Molybdenum |
2.00-3.00 |
2.00-3.00 |
|
Nitrogen |
≤0.10 |
≤0.10 |
|
Iron |
Balance |
Balance |
Mechanical Properties
|
Grades |
Tensile Strength ksi(Mpa), min. |
Yield Strength, ksi(Mpa) |
Elongation, % |
Hardness, Rockwell |
|
SS316 |
84(579) |
42(290) |
50 |
B79 |
|
SS316L |
81(558) |
42(290) |
50 |
B79 |
Application
Chemical: chemical containers, pressure vessels, and industrial equipment
Water treatment: woven or welded screens for water filtration
Pulp and paper: used in paper machines to avoid iron contamination.
Automotive: threaded fasteners, springs, and furnace parts
Medical: medical equipment and orthopedic implants
Dental: dental implants, orthodontic appliances, and various dental instruments
Semiconductor: semiconductor manufacturing equipment and cleanroom environments
Food processing: food preparation surfaces, equipment, and appliances
Aerospace: aircraft structures, fasteners, turbine blades, and exhaust systems
Surface Treatment

Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.