2205 Duplex Stainless Steel Pipe (UNS S31803)

2205 Duplex Stainless Steel Pipe (UNS S31803)

UNS S31803 Duplex Pipe has high resistance to chloride stress corrosion cracking,resistance to chloride pitting and crevice corrosion,good general corrosion resistance
Send Inquiry

UNS S31803 Duplex Stainless Steel Pipes & Tubes

 

– Premium Corrosion-Resistant Solutions by Lork Group

Superior Performance of UNS S31803 Duplex Pipes & Tubes

Lork Group is a trusted global supplier of high-quality UNS S31803 duplex stainless steel pipes and tubes, offering an exceptional combination of high strength and corrosion resistance. As the most widely used duplex grade, UNS S31803 provides twice the yield strength of standard austenitic stainless steels while maintaining excellent resistance to stress corrosion cracking and pitting.

Key Characteristics & Advantages

  • Exceptional Corrosion Resistance - Outstanding performance in chloride, sour, and acidic environments
  • High Mechanical Strength - Yield strength approximately 2x higher than 316L stainless steel
  • Stress Corrosion Cracking Resistance - Ideal for harsh oil & gas and chemical processing applications
  • Good Weldability & Fabrication Properties - Suitable for complex piping systems and pressure vessels
  • Cost-Effective Solution - Lower nickel content than austenitic grades provides better value

Note: Not recommended for continuous service above 300°C due to potential embrittlement

 

Specification

 

Type

Cold Drawn / Welded / ERW

Outer Diameter Size

Seamless - 1/4" NB to 6" NB (Nominal Bore Size)
Welded / ERW- 1" NB to 16" NB (Nominal Bore Size)

Wall Thickness

Schedule 10 to Schedule 160

Length

5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.

Ends

Plain Ends / Beveled Ends

Delivery Conditions

As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered

Coating

Electropolish, Mechanical Polish, Satin Finish, Passivated

Other Testing

NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc.

Dimension

All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME

Value Added Services

Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment

Packaging

Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector

 

Chemical Composition

 

Element

Content (%)

Iron, Fe

63.75-71.92

Chromium, Cr

21.0-23.0

Nickel, Ni

4.50-6.50

Molybdenum, Mo

2.50-3.50

Manganese, Mn

2.0

Silicon, Si

1.0

Nitrogen, N

0.080-0.20

Carbon, C

0.030

Phosphorous, P

0.030

Sulfur, S

0.020

 

Physical Properties

 

Properties

Metric

Imperial

Density

7.82 g/cm³

0.283 lb/in³

 

Mechanical Properties

 

Properties

Metric

Imperial

Tensile strength at break

621 MPa

90000 psi

Yield strength (@strain 0.200 %)

448 MPa

65000 psi

Elongation at break (in 50 mm)

25.0 %

25.0 %

Hardness, Brinell

293

293

Hardness, Rockwell c

31.0

31.0

 

Industrial Applications

 

UNS S31803 duplex pipes and tubes are extensively used in demanding environments:

Oil & Gas Industry

  • Subsea pipelines and flowlines
  • Downhole tubing and casings
  • Process piping and heat exchangers

Chemical Processing

  • Acid production equipment
  • Chemical transport piping
  • Pressure vessels and reactors

Pulp & Paper Industry

  • Digester vessels
  • Bleach plant washers
  • Chip pre-steaming systems

Other Key Applications

  • Desalination plants
  • Flue gas cleaning systems
  • Food processing equipment
  • Structural components in marine environments

Hot Tags: UNS S31803, Duplex Pipe, 2205 Duplex, ASTM A790, 22Cr Duplex, Ferritic-Austenitic Pipe, High Strength Pipe, Chloride Resistant Pipe

Send Inquiry