316/316L Stainless Steel Strip
Lork Group is a reliable manufacturer and supplier of 316 316L Stainless Steel Strip and Coil in China. Type 316 is an austenitic chromium-nickel-stainless steel containing molybdenum. This addition increases general corrosion resistance, improves resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures.
316 316L Stainless Steel Strip properties are similar to those of Type 304/304L except that this alloy is somewhat stronger at elevated temperatures. Corrosion resistance is improved, particularly against sulfuric, hydrochloric, acetic, formic and tartaric acids; acid sulfates and alkaline chlorides.
Type 316L is an extra-low carbon version of Type 316 that minimizes harmful carbide precipitation during welding.
As a leading Stainless Steel strip and coil supplier in China, Lork Group manufactures and produces 316 316L Stainless Steel Strip of various sizes. If you have any mechanical requirements, please confirm with we. We can customize the material exactly to your requirements.
Chemical Composition
|
Element |
% |
|
C |
0.07 max |
|
Mn |
2.00 max |
|
Si |
1.00 max |
|
P |
0.045 max |
|
S |
0.030 max |
|
Cr |
16.5 – 18.0 |
|
Ni |
10.5 – 13.5 |
|
N |
0.10 max |
|
Mo |
2.00 – 2.50 |
|
Fe |
Balance |
Physical Properties
|
Density |
g/cm³ |
8.00 |
|
lb/in.³ |
0.285 |
|
|
Modulus of Elasticity (E) |
At 70°F (20°C) |
28.0 x 10³ ksi (193 GPa) |
|
Modulus of Rigidity (G) |
At 70°F (20°C) |
10.1 x 10³ ksi (70 GPa) |
|
Electrical Resistivity |
29.1 µohm-in, (74 µohm-cm) |
|
|
Thermal Conductivity |
9.4 Btu-in/ft2hr-°F, (212°F) |
|
|
Coefficient of Expansion |
9.2 µin/in.-°F (70-212°F) |
|
|
16.6 µm/m-°C (200-100°C) |
||
Mechanical Properties
|
Annealed |
Heat Treatment |
1900-2050°F (1038-1121°C) |
|
Tensile Strength |
75 – 105 ksi (515-725 MPa) |
|
|
Suggested Operating Conditions |
-200°F to 1700°F (-184°C to 927°C) |
|
|
1/4 Hard |
Heat Treatment |
(Stress relieve 600-900°F as needed) |
|
Tensile Strength |
125 ksi min (860 MPa) |
|
|
Suggested Operating Conditions |
-200°F to 550°F (-184°C to 288°C) |
|
|
1/2 Hard |
Heat Treatment |
(Stress relieve 600-900°F as needed) |
|
Tensile Strength |
150 ksi min (1030 MPa) |
|
|
Suggested Operating Conditions |
-200°F to 550°F (-184°C to 288°C) |
|
|
Spring Temper |
Heat Treatment |
(Stress relieve 600-900°F as needed) |
|
Tensile Strength |
185 ksi min (1275 MPa) |
|
|
Suggested Operating Conditions |
-200°F to 550°F (-184°C to 288°C) |
Application
- Exhaust manifolds
- Furnace parts
- Heat exchangers
- Jet engine parts
- Pharmaceutical and photographic equipment
- Valve and pump trim
- Tubing
- Chemical equipment
- Digesters
- Tanks
- Evaporators
- Paper and textile processing equipment
- Food processing equipment
- Marine parts.
Surface Treatment

Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.
Hot Tags: 316/316l stainless steel strip, China 316/316l stainless steel strip manufacturers, factory
You Might Also Like