347 Stainless Steel Strip (UNS S34700)

347 Stainless Steel Strip (UNS S34700)

347 Stainless Steel Strip has excellent resistance to oxidation, even surpassing that of 321 in strong oxidizing conditions. The alloy maintains resistance to intergranular corrosion, while also possessing good creep strength compared to other 300 series stainless steels.
Send Inquiry

Lork Group is a reliable manufacturer and supplier of 347 Stainless Steel Strip and Coil in China. Type 347 is a stabilized austenitic stainless steel, similar to type 304, but alloyed with Niobium (Columbium) for use in applications involving continuous or intermittent service at 800-1500°F (427-816°C).

 

347 Stainless Steel Strip has excellent resistance to oxidation, even surpassing that of 321 in strong oxidizing conditions. The alloy maintains resistance to intergranular corrosion, while also possessing good creep strength compared to other 300 series stainless steels. The alloy is strengthened only through cold work and can be fabricated, machined, and welded via most conventional processes.

 

As a leading Stainless Steel strip and coil supplier in China, Lork Group manufactures and produces 347 Stainless Steel Strip of various sizes. If you have any mechanical requirements, please confirm with we. We can customize the material exactly to your requirements.

 

Chemical Composition

 

Element

%

C

0.08 max

Mn

2.00 max

Si

1.00 max

P

0.045 max

S

0.030 max

Cr

17.0 – 19.0

Ni

9.0 – 12.0

Nb(Cb)

10*C – 1.00

N

0.10 max

Fe

Balance

 

Physical Properties

 

Density

g/cm³

7.96

lb/in.³

0.288

Modulus of Elasticity (E)

At 70°F (20°C)

28.0 x 10³ ksi (193 GPa)

Modulus of Rigidity (G)

At 70°F (20°C)

11.2 x 10³ ksi (78 GPa)

Electrical Resistivity

28.4 µohm-in, (72 µohm-cm)

Thermal Conductivity

113 Btu-in/ft2hr-°F, (212°F)
16.3 W/m-°C (100°C)

Coefficient of Expansion

11.4 µin/in.-°F (32-1500°F)

20.5 µm/m-°C (0-871°C)

 

Mechanical Properties

 

Annealed

Heat Treatment

1750-2150°F (954-1175°C)

Tensile Strength

90 – 110 ksi (620-760 MPs)

Suggested Operating Conditions

up to 1500°F (816°C)

 

Application

 

  • Annealing covers
  • High-temperature tempering equipment
  • Diesel and heavy-duty automotive exhaust
  • Firewalls
  • Stack liners
  • Boiler casings
  • Welded pressure vessels
  • Aircraft components
  • Bellows
  • Oil refinery equipment
  • Springs

 

Surface Treatment

 

product-1200-750

 

Hot Tags: 347 Stainless Steel, 347 Strip, Stainless Steel Strip, UNS S34700, Niobium-stabilized stainless steel, Austenitic stainless steel strip, Aerospace strip

Send Inquiry