• Stellite 6 Cobalt Rod

    Stellite 6 is a cobalt-based superalloy known for its exceptional wear resistance, high-temperature strength, and corrosion resistance.

  • Stellite 6 Plate / Sheet

    Stellite 6 plates—a cobalt-chromium-tungsten (Co-Cr-W) hardfacing alloy. This material features high hardness and excellent wear and galling resistance. It is available in hot-rolled/forged and

  • Stellite 6B Plate / Sheet(UNS R30016)

    Stellite 6B Plate/Sheet (UNS R30016) is a wrought cobalt-chromium-tungsten wear-resistant alloy plate suitable for high-temperature wear applications such as turbine blade shrouds, wear liners,

  • AMS 5894 Stellite 6B Cobalt Alloy

    Stellite 6B (AMS 5894) is an aerospace-grade wrought cobalt alloy featuring excellent wear resistance, galling resistance, and high-temperature hardness. It meets the requirements of the AMS 5894

  • X40 Stellite 31

    Stellite 31 (X40) is a cast cobalt-based superalloy used for hot-section components in gas turbines. Standard bar sizes range from 4mm to 600mm in diameter, priced at $65–$80 per kilogram; custom

  • Stellite 12 Plate

    Stellite 12 (UNS R30012) is a medium-to-high carbon cobalt-chromium-tungsten hard-facing alloy available in the form of cold-rolled sheets and hot-rolled plates; inquiries are welcome.

  • Stellite 21 Cobalt Bar

    It is the toughness champion of the Stellite family; rather than striving for maximum hardness, it achieves an optimal balance of impact resistance, thermal fatigue resistance, and corrosion

  • Stellite 1 Bar(UNS R30001)

    Stellite 1 bar (UNS R30001) is a high-carbon cobalt-chromium-tungsten alloy rod designed for extreme wear conditions. Standard sizes ranging from Ф4mm to Ф600mm are available for immediate shipment.

  • Stellite 4 Bar(UNS R30004)

    Stellite 4 bar is a high-carbon, high-tungsten cobalt-based alloy available in diameters ranging from Ф4 mm to Ф600 mm. Surface finishes include turned, ground, or black (as-forged/as-cast),

  • Stellite 1 Pipe(UNS R30001)

    Stellite 1—a cobalt-based alloy—is currently priced at a market reference of $60–100/kg (MOQ: 100 kg). It offers excellent wear and galling resistance, making it an ideal choice for valve seats, pump

  • Stellite 3 Pipe(UNS R30003)

    Stellite 3 pipe is a high-carbon cobalt-based hardface alloy tubing with excellent wear resistance, a hot hardness of up to 800°C, and oxidation resistance up to 1000°C. Customization services are

  • Stellite 12 Cobalt Alloy Bar

    It represents the advanced tier of the Stellite family: featuring a carbon content of 1.4%, a hardness of HRC 45–51, and a high tungsten content, it offers excellent high-temperature resistance.

Send Inquiry