• Monel 400 Copper Nickel Alloy Sheet

    Monel 400 Plate is a copper-nickel alloy made metallic plate. Monel 400 Plate has good ductility and corrosion resistance to a variety of corrosive media.

  • Hastelloy G-35 Nickel Alloy(ASTM B575)

    Hastelloy G-35 is a high-performance nickel-chromium-iron-molybdenum alloy designed to resist extreme corrosion in highly oxidizing, highly reducing and mixed acid environments. ASTM B575 Hastelloy

  • ASTM B168 Inconel 693 Nickel Alloy

    Inconel 693 is a high-nickel-chromium alloy that is resistant to high-temperature corrosion, with high-temperature oxidation resistance being key. Lork Group typically supplies ASTM B168 Inconel 693

  • Haynes HR160 Nickel Alloy(W.Nr.2.4880)

    Haynes HR160 has strong resistance to sulfidation in both oxidizing and reducing atmospheres, making it an ideal material for manufacturing waste incinerators. The W.Nr.2.4880 Haynes HR 160 Nickel

  • W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip

    W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip is a nickel-molybdenum alloy designed to address corrosion issues in strongly reducing media. It offers excellent resistance to reducing

  • Titanium 6al-6v-2sn Alloy

    Lork Group is currently offering Titanium 6Al-6V-2Sn Alloy. We offer precision machining, a variety of specifications, and support third-party testing. Get a quick quote today!

  • 2.4654 / UNS N07001 / Waspaloy Sheet

    Lork Group is a premier international exporter and supplier of AMS 5544 Waspaloy (UNS N07001), the premium nickel-based superalloy renowned for its exceptional strength and corrosion resistance at

  • Hastelloy G-30 Nickel Sheet(UNS N06030)

    Lork Group is a leading international exporter and stockist of Hastelloy G30 (UNS N06030) nickel sheets, providing superior corrosion-resistant solutions for demanding industrial applications

  • UNS N0645 / Hastelloy C4 Nickel Sheet

    Hastelloy C-4 was designed to address the most critical drawback of Hastelloy C-276: thermal stability. The composition of C-4 has been specifically optimized so that, even without post-weld solution

  • Hastelloy B-2 Nickel Plate(ASTM B575)

    Lork Group is a trusted global exporter and supplier of Hastelloy B-2 (UNS N10665 / 2.4617), the specialized nickel-molybdenum alloy renowned for its exceptional resistance to the most severe

  • Incoloy 901 Nickel Alloy

    Lork Group offers Incoloy 901 nickel alloy in a variety of specifications. We support custom nickel alloy processing and provide fast quotes!30kg $25-$30 MOQ50-100kg $20-$25 100-500kg $15-$20

  • Inconel 706 Nickel Alloy Sheet (AMS 5605)

    Lork Group supplies high-quality Inconel 706 Nickel Alloy in Rod, Bar, Plate, Sheet, Strip & Wire forms. AMS 5605 certified. Request free samples & competitive pricing today!

We're well-known as one of the leading plate and sheet manufacturers in China. Please feel free to buy cheap plate and sheet for sale here and get pricelist from our factory. For price consultation, contact us.

Send Inquiry