W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip

W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip

W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip is a nickel-molybdenum alloy designed to address corrosion issues in strongly reducing media. It offers excellent resistance to reducing acids such as hydrochloric acid and sulfuric acid. It is a specialized material for the chemical industry.
Send Inquiry

 

W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip Description

 

W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip is extremely resistant to reducing media and localized corrosion. However, due to its extremely low chromium content, Hastelloy B-2 is not resistant to oxidizing media (such as nitric acid and solutions containing Fe⁺ or Cu⁺ ions).

 

Two key considerations when purchasing W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip:


1. Strictly avoid oxidizing environments:

This is the primary principle when selecting materials. Ensure that the medium is free of oxidizing substances.

 

2. Pay attention to medium-temperature brittleness:

Prolonged exposure to temperatures between 600-900°C can cause brittle phase precipitation in W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip, making the material brittle. For components subject to medium- to long-term high-temperature service, consider evaluating the improved Hastelloy B-3 alloy, which offers improved thermal stability.

 

If you are interested in W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip, please click the circle icon below to initiate an online communication.

 

 

W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip Parameters

 

 

 

 Hastelloy B-2 Nickel Alloy stock

Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft nickel alloys for you!.
Bar 2

Hastelloy B-2 Bar

Specifications

UNS N10665
W.Nr. 2.4617
ASTM B335
Plate 1

Hastelloy B-2 Plate

Specifications

UNS N10665
W.Nr. 2.4617
ASTM B333
Pipe 1

Hastelloy B-2 Pipe

Specifications

UNS N10665
W.Nr. 2.4617
ASTM B622
Coil 1

Hastelloy B-2 Strip

Specifications

UNS N10665
ASTM B564
ASTM B333

 

Hastelloy B-2 Nickel Alloy Strip Manufacturing and Pricing Reference

 

 

Hastelloy B-2 Nickel Alloy Strip

   Cold Working:

   This alloy exhibits a high work-hardening rate. Cold working (e.g., cold bending, cold rolling) may require lower cutting speeds and greater feeds than those used for stainless steel, and intermediate annealing may be required between passes to soften the material.

   Machining:

   Machining should be performed in the annealed condition using sturdy machine tools and sharp carbide tools.

     Lork Group offers customized W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip. The approximate prices for W.Nr. 2.4617 / ASTM B333 Hastelloy B-2 Nickel Alloy Strip offered by Lork Group are:
1. Stock Material: $18/kg (MOQ 30kg), $15/kg (100kg)
2. Processing: Cutting, chipping, milling, etc. (Price based on material loss and processing method)
3. Custom Material - Metallurgy, heat treatment, and other solutions available (Price based on your requirements)
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

hastelloy b2

 

 The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information! 

 

 

Hastelloy B-2 Nickel Alloy Chemical Composition

 

Weight% Hastelloy B-2
Mn 1.0
Cr 0.4 - 0.7
Mo 26.0 - 30.0
Ti 2.9
Fe 1.6 - 2.0
Cu 0.5 max
Mn/Si/Al/C/S Trace
Ni Bal

 

 

Hastelloy B-2 Nickel Alloy Mechanical Properties

 

Material Hastelloy B-2
Tensile Strength ksi 110
Yield Strength ksi 51
Reduction of Area % 40
Hardness HB ≤ 230 HB

 For more Incoloy 901 Nickel Alloy details, please contact us!

 

Contact now

 

Hot Tags: w.nr. 2.4617 / astm b333 hastelloy b-2 nickel alloy strip, China w.nr. 2.4617 / astm b333 hastelloy b-2 nickel alloy strip manufacturers, factory