AISI 904L Stainless Steel Pipe (UNS N08904,ASTM A312)

AISI 904L Stainless Steel Pipe (UNS N08904,ASTM A312)

Lork Group is a leading international exporter and supplier of high-performance ASTM A312 AISI 904L Stainless Steel Pipes. We supply a comprehensive range of both seamless and welded 904L stainless steel pipes.
1. Standard: ASTM A312 / ASME SA312、ASTM A213/ASME SA213、ASTM B677 / ASME SB677
2. Size: 1/2”- 48”
3. Thickness: 0.5mm-30mm
4. 904L stainless steel pipe price: 15-25 $
Send Inquiry

Lork Group - Your Trusted Exporter for ASTM A312 904L / 1.4539 Stainless Steel Pipes

Lork Group is a leading international exporter and supplier of high-performance ASTM A312 AISI 904L Stainless Steel Pipes. Also known by the designations UNS N08904 and Werkstoff Nr. 1.4539, this super austenitic alloy is engineered for exceptional resistance to severe corrosive environments. Perfect for critical applications in chemical processing, petrochemical, pharmaceutical, and offshore industries. Our products meet international standards, including ASTM A312, ASME SA312, and ASTM B677.

ASTM A312 ASME SA312
ASTM A312 / ASME SA312
The primary standard for seamless, welded, and heavily cold-worked austenitic stainless steel pipes. It mandates strict requirements for chemical composition, mechanical properties, and heat treatment.
ASTM A213 ASME SA213
ASTM A213 / ASME SA213
Covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes, often applicable for pressure vessel applications.
ASTM B677 ASME SB677
ASTM B677 / ASME SB677
A standard dedicated specifically to UNS N08904 (904L), UNS N08925, and UNS N08926 seamless pipe for general corrosion service, emphasizing its unique properties.
ASME B3619
ASME B36.19
Defines the standard dimensions for stainless steel pipe.

 

ASTM A312 904L Stainless Steel Pipe Specifications

 

Specifications ASTM A 312 / ASME SA 312
ASTM B677 / ASME SB 677
Dimensions ASTM, ASME, and API
SS 904L Pipes 1/2″ NB – 16″ NB
ERW 904L Pipes 1/2″ NB – 24″ NB
EFW 904L Pipes 6″ NB – 100″ NB
Size 1/8″NB TO 30″NB IN
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Type Seamless / ERW / Welded / Fabricated / LSAW Pipes
Length Single Random, Double Random & Cut Length.
End Plain End, Beveled End, Threaded

 

AISI 904L Steel Pipe Size

 

OD mm. NPS in. WT mm. Sch Kg/m
13.72 0.25 1.65 10S 0.5
2.24 40S 0.64
3.02 80S 0.81
17.15 0.375 1.65 10S 0.64
2.31 40S 0.86
3.2 80S 1.12
21.34 0.5 2.11 10S 1.02
2.77 40S 1.29
3.73 80S 1.65
26.67 0.75 2.11 10S 1.3
2.87 40S 1.71
3.91 80S 2.23
33.4 1 2.77 10S 2.13
3.38 40S 2.54
4.55 80S 3.29
6.352) 160S 4.3
42.16 1¼ 2.77 10S 2.73
3.56 40S 3.44
4.85 80S 4.53
6.352) 160S 5.69
48.26 1½ 2.77 10S 3.16
3.68 40S 4.11
5.08 80S 5.49
60.33 2 2.77 10S 3.99
3.91 40S 5.52
5.54 80S 7.6
8.742) 160S 11.29
73.03 2½ 3.05 10S 5.35
5.16 40S 8.77
7.01 80S 11.59
88.9 3 3.05 10S 6.56
5.49 40S 11.47
7.62 80S 15.51
11.132) 160S 21.67
101.6 3½ 3.05 10S 7.53
5.74 40S 13.78
8.08 80S 18.92
114.3 4 3.05 10S 8.5
6.02 40S 16.32
8.56 80S 22.67
13.492) 160S 34.05
141.3 5 6.55 40S 22.1
9.53 80S 31.44
15.882) 160S 49.87
168.28 6 3.4 10S 14.04
7.11 40S 28.69
10.97 80S 43.21
18.262) 160S 68.59
219.08 8 8.18 40S 43.2
12.7 80S 65.63
23.012) 160S 112.97

 

1.4539 AISI 904L Chemical Properties

 

Grade Cr Ni C Si Mn P S Mo Cu Fe
AISI 904L min: 19
max: 23
min: 23
max: 28
0.02 Max 1.0 max 2.0 max 0.045 max 0.035 max min: 4
max: 5
min: 1
max: 2
balance

 

Mechanical Properties

 

Grade Tensile Strength (MPa) min Elongation (% in 50mm) min Yield Strength 0.2% Proof (MPa) min Hardness
Rockwell B (HR B) max Brinell (HB) max
AISI 904L 490 35 220 70-90 typical -

 

Manufacturing and Quality Assurance

 

To ensure every length of pipe meets the highest standards of integrity and performance, manufacturers adhere to a stringent quality protocol:

 

1. Heat Treatment: All 1.4539 stainless steel pipe is supplied in a solution-annealed condition. This process involves heating the material to a specific temperature (typically 1100-1170°C) followed by rapid quenching. This treatment dissolves any secondary phases (like carbides) that can impair corrosion resistance and restores the material's ductility.

 

2. Comprehensive Testing Regime: Each production batch undergoes a battery of tests to verify its properties:

Mechanical Testing:

  • Transverse or Longitudinal Tensile Test: Measures ultimate tensile strength, yield strength, and elongation.

Non-Destructive Testing (NDT):

  • Hydrostatic Pressure Test: Verifies the integrity of the pipe under pressure.
  • Ultrasonic Test (UT) / Electromagnetic Test: Detects internal and surface imperfections.
  • X-Ray Flaw Detection: Provides a detailed internal inspection, especially critical for welded pipes.

Corrosion Testing: Specific tests may be conducted to validate performance in simulated service environments.

Formability Testing:

  • Flattening Test: Assesses the ductility and soundness of the weld in welded pipes by flattening a ring sample until the walls meet.

 

Applications

 

Due to its robust properties, ASTM A312 904L pipe is specified for the most challenging applications:

  • Chemical processing reactors and piping systems (handling sulfuric, phosphoric, and acetic acids)
  • Seawater cooling systems and components in desalination plants
  • Pulp and paper digesters and bleach plants
  • Pollution control and flue gas desulfurization (FGD) systems
  • Pharmaceutical and food processing equipment where high purity and corrosion resistance are required

 

We stock a vast range of sizes from 1/2" to 48" with wall thicknesses from 0.5mm to 30mm. All our pipes undergo rigorous testing, including hydrostatic, ultrasonic, X-ray, and flattening tests, ensuring they deliver superior mechanical properties and corrosion resistance.

 

Contact Lork Group now for competitive pricing, detailed product information, and a free, no-obligation quotation. Let our expertise in exporting high-quality ASTM A312 904L stainless steel pipes provide the solution for your most challenging applications.

 

Contact now

 

Hot Tags: 904L Pipe, AISI 904L, 1.4539, UNS N08904, ASTM A312, sulfuric acid resistant pipe, super austenitic pipe, seawater pipe, chemical pipe, 904L

Send Inquiry