• Stellite 12 Cobalt Alloy Bar

    It represents the advanced tier of the Stellite family: featuring a carbon content of 1.4%, a hardness of HRC 45–51, and a high tungsten content, it offers excellent high-temperature resistance.

  • AMS 5544 Waspaloy Alloy Sheet

    AMS 5544 Waspaloy Alloy Sheet is a nickel based age hardenable alloy that possesses high temperature strength while still having a good corrosion resistance, especially to oxidation.

  • AMS 5581 Inconel 625 Nickel Alloy

    Its core competitive advantage lies in the combination of niobium solid-solution strengthening and molybdenum corrosion resistance. It is easy to weld and suitable for use across a wide temperature

  • AMS 5510 321 Stainless Steel Sheet

    For applications susceptible to intergranular corrosion—such as aircraft exhaust systems, petrochemical boiler heat exchangers, and welded pressure vessels—Grade 321 stainless steel stands as a

  • MP159 Cobalt Alloy Pipe (UNS R30159)

    MP159 pipe has excellent strength and ductility in temperatures up to 1100- 1200° F. Has stress corrosion and corrosion resistant to crevice corrosion and hydrogen.

  • AMS 5581 / Inconel 625 Seamless Tube

    Our manufactured sizing capabilities for Inconel 625 seamless tube and pipe ranges from 2-1/16” to 10-3/4” OD with wall thicknesses up to 1.925”. Please reach out for more information on our minimum

  • AMS 5555 / UNS N02205 / Nickel 205 Wire

    Nickel 205 alloy contains small additions of aluminum and titanium for a good combination of mechanical and electrical properties. Contact Lrok Group today for Nickel 205 alloy specifications,

  • AMS 5876 / UNS R30003 / Elgiloy Material

    Lork Group is a trusted supplier of high-performance Elgiloy Alloy (AMS 5876 / UNS R30003), providing premium-quality cobalt-chromium-nickel-molybdenum strips, wires, and precision components. Our

  • UNS K93120 / AMS 6514 Maraging 300 Steel

    Maraging 300 (18Ni300 / UNS K93120) is an ultra-low-carbon nickel-cobalt-molybdenum-titanium maraging steel available in various forms—such as bars, plates, tubes, and strips—and complies with the

  • Haynes 188 Cobalt Alloy Pipe (UNS R30188)

    Haynes 188 pipe is a cobalt-base superalloy with a unique combination of high oxidation resistance, along with adequate ductility after prolonged exposure to the 1400-1600 °F temperature range.

  • Nitronic 40 Round Bar(AMS 5656 / AMS 5595)

    Lork Group is a trusted supplier of high-quality Nitronic 40 (AMS 5656 / AMS 5595) round bar, providing premium austenitic stainless steel for aerospace, chemical processing, and cryogenic

  • AMS 5598 / Inconel X750 Nickel Alloy Strip

    Inconel X750 (AMS 5598) nickel alloy strip is a nickel-chromium alloy X750 for aerospace, nuclear, and industrial applications. Request a free quote today!

Send Inquiry