Nitronic 40 Round Bar(AMS 5656 / AMS 5595)

Nitronic 40 Round Bar(AMS 5656 / AMS 5595)

Lork Group is a trusted supplier of high-quality Nitronic 40 (AMS 5656 / AMS 5595) round bar, providing premium austenitic stainless steel for aerospace, chemical processing, and cryogenic applications. Our Nitronic 40 round bars deliver exceptional strength, corrosion resistance, and non-magnetic properties, making them ideal for demanding environments.
Send Inquiry

A High-Performance Austenitic Stainless Steel for Demanding Applications

Nitronic 40 (AMS 5656 / AMS 5595) round bar is a premium-grade austenitic stainless steel renowned for its exceptional strength, corrosion resistance, and high-temperature performance. With a unique composition of 21% chromium, 6% nickel, and 9% manganese, this nitrogen-strengthened alloy delivers superior mechanical properties in the annealed condition while maintaining excellent fabricability and weldability.

Key Properties of Nitronic 40 (AMS 5656 / AMS 5595) Round Bar

Cryogenic Toughness

– Maintains structural integrity in extremely low-temperature environments.

High Strength in Annealed Condition

– Offers greater yield and tensile strength compared to conventional stainless steels like 304 and 316.

Outstanding Corrosion Resistance

– Resists oxidation at elevated temperatures and performs well in harsh chemical environments.

Non-Magnetic

– Remains nonmagnetic even after severe cold working, making it ideal for sensitive applications.

Excellent Fabricability

– Can be machined, formed, and welded using techniques similar to 300-series stainless steels.

 

Specifications & Standards

Nitronic 40 round bar complies with multiple industry standards, including:

AMS 5656 (Bar, Wire, Rings, Extrusions)

AMS 5595 (Sheet, Plate, Strip)

ASTM A276 / ASME SA276 (Stainless Steel Bars)

ASTM A412 / ASME SA412 (Seamless & Welded Tubes)

UNS S21906 – Unified Numbering System designation

 

Chemical Composition

Weight% C P Si Ni Fe Mn S Cr N Mo Cu
Nitronic 40 (21-6-9) 0.04 max 0.060 max 1.00 max 5.5-7.5 Bal 8-10 0.030 max 19-21.5 0.15-0.40 0.75 max 0.75 max

 

Typical Mechanical Properties

Alloy Cross Section Size Test Direction Yield Strength 0.2% Ultimate Tensile Strength Elongation in 2"(%) Reduction of Area % Rockwell B Hardness
ksi MPa ksi MPa
Nitronic 40 (21-6-9) 6" (152mm) sq Longitudinal 62 428 95 655 46 69  
Nitronic 40 (21-6-9) 6" (152mm) sq Transverse 52 358 93 641 30 45  
Nitronic 40 (21-6-9) 4" (102mm) sq Longitudinal 56 386 97 668 53 73  
Nitronic 40 (21-6-9) 1" (25.4mm)sq Longitudinal 52 358 101 696 53 73 90

 

Applications of Nitronic 40 Round Bar

Due to its robust properties, Nitronic 40 (AMS 5656 / AMS 5595) round bar is widely used in:

  • Aerospace & Defense – Aircraft engine components, ducting, and bellows
  • Chemical Processing – Equipment exposed to corrosive media
  • Cryogenic Systems – Components requiring low-temperature durability
  • Marine & Offshore – High-strength, corrosion-resistant fasteners and fittings

 

Why Choose Nitronic 40 Round Bar?

For engineers and manufacturers seeking a high-performance stainless steel that balances strength, corrosion resistance, and ease of fabrication, Nitronic 40 (AMS 5656 / AMS 5595) round bar is an outstanding choice. Its versatility makes it a preferred material for critical applications across aerospace, chemical, and cryogenic industries.

 

Whether for precision machining, structural components, or high-stress environments, Nitronic 40 delivers unmatched reliability and longevity. For high-quality round bar stock meeting stringent AMS and ASTM specifications, this alloy stands as a top-tier engineering solution.

 

Lork Group is a trusted supplier of high-quality Nitronic 40 (AMS 5656 / AMS 5595) round bar, providing premium austenitic stainless steel for aerospace, chemical processing, and cryogenic applications. Our Nitronic 40 round bars deliver exceptional strength, corrosion resistance, and non-magnetic properties, making them ideal for demanding environments.

 

Why Choose Lork Group for Nitronic 40 Round Bar?

  • High-Quality Material – Fully compliant with AMS 5656, AMS 5595, ASTM A276, and ASME SA276 standards.
  • Competitive Pricing – Cost-effective solutions without compromising performance.
  • Global Supply – Reliable logistics and on-time delivery worldwide.
  • Technical Support – Expert guidance on material selection and application suitability.

 

Contact Lork Group today for Nitronic 40 round bar specifications, pricing, and availability! Get a fast quote and discover why leading industries trust us for high-performance stainless steel solutions.

Email: susan@lorkgroup.com
WhatsApp: +86 19937075488

Contact now

 

 

Hot Tags: Nitronic 40 Bar, Nitronic 40 round bar, UNS S21900, XM-10,21-6-9, Austenitic Stainless, Nitronic 40 Bar supplier, AMS 5656, AMS 5595

Send Inquiry