Incoloy 864 Alloy Pipe
Incoloy 864 alloy pipe (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stress-corrosion cracking.
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
30 - 38 |
|
Iron, Fe |
29.105 - 45 |
|
Chromium, Cr |
20 - 25 |
|
Molybdenum, Mo |
4 - 4.8 |
|
Silicon, Si |
0.60 - 1 |
|
Titanium, Ti |
0.40 - 1 |
|
Carbon, C |
≤ 0.080 |
|
Sulfur, S |
≤ 0.015 |
Physical Properties
|
Properties |
Metric |
Imperial |
|
Density |
8.02 g/cm3 |
0.290 lb/in3 |
|
Melting point |
1353-1393°C |
2467-2539°F |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile strength |
648 MPa |
94000 psi |
|
Yield strength |
109.6 MPa |
15900 psi |
|
Elongation at break |
16.60% |
16.60% |
Thermal Properties
|
Properties |
Metric |
Imperial |
|
Thermal expansion co-efficient (@100°C/212°F) |
14.7 µm/m°C |
8.17 µin/in°F |
|
Thermal conductivity (@23°C/73.4°F) |
11 W/mK |
76.3 BTU.in/hrft².°F |
Incoloy 864 Alloy Pipe Applications
- Automotive exhaust system
- EGR tubes
- Tailpipes
- Manifolds
Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.
Hot Tags: incoloy 864 alloy pipe, China incoloy 864 alloy pipe manufacturers, factory
You Might Also Like
Send Inquiry