Incoloy 800HT Nickel Alloy Pipe (UNS N08811)

Incoloy 800HT Nickel Alloy Pipe (UNS N08811)

Incoloy 800HT nickel alloy exhibits excellent stress-rupture strength. Produced via seamless welding and compliant, it is ideally suited for reformer and cracking furnace operations.
Send Inquiry

Incoloy 800HT is a high-temperature, nickel-iron-chromium alloy with excellent oxidation and carburization resistance. It is a modified version of Incoloy 800, with tighter chemical composition controls and enhanced high-temperature strength due to increased titanium and aluminum content. Incoloy 800HT pipes are ideal for extreme heat and corrosive conditions, making them a top choice for industries requiring durable, high-performance piping solutions

 

Key Features of Incoloy 800HT Pipes

 

  • High-Temperature Resistance: Performs well in temperatures up to 1500°F (815°C).
  • Corrosion Resistance: Resistant to oxidation, carburization, and sulfidation in harsh environments.
  • Mechanical Strength: Maintains strength and creep resistance at elevated temperatures.

 

Specification

 

Type

Cold Drawn / Welded / ERW

Outer Diameter Size

Seamless - 1/4" NB to 6" NB (Nominal Bore Size)
Welded / ERW- 1" NB to 16" NB (Nominal Bore Size)

Wall Thickness

Schedule 10 to Schedule 160

Length

5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size.

Ends

Plain Ends / Beveled Ends

Delivery Conditions

As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered

Coating

Electropolish, Mechanical Polish, Satin Finish, Passivated

Other Testing

NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved, etc.

Dimension

All pipes are manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME

Value Added Services

Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment

Packaging

Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector

 

Chemical Composition

 

Elements

Content (%)

Iron, Fe

≥ 39.5

Nickel, Ni

30- 35

Chromium, Cr

19-23

Manganese, Mn

≤ 1.50

Silicon, Si

≤ 1

Copper, Cu

≤ 0.75

Titanium, Ti

0.15-0.60

Aluminum, Al

0.15-0.60

Carbon, C

0.060-0.10

Sulfur, S

≤ 0.015

 

Mechanical Properties

 

Properties

Metric

Imperial

Tensile strength (annealed)

560 MPa

81200 psi

Yield strength (annealed)

250 MPa

36300 psi

Elongation at break (annealed prior to test)

45%

45%

 

Application

 

  • Hydrocarbon cracking
  • Industrial furnace and boiler components and equipment
  • Equipment for Heat-Treating
  • Pressure vessels and heat exchangers
  • Chemical and Petrochemical processing

 

Hot Tags: Incoloy 800HT, Alloy 800HT, Nickel Pipe, UNS N08811, creep-resistant pipe, oxidation-resistant pipe, petrochemical pipe, furnace tube material