Inconel 625 Nickel Alloy Pipe (UNS N06625)
Lork Group is a leading supplier and exporter of the Inconel 625 Pipe and tubes. Alloy 625 Seamless Pipe is a nickel chromium super alloy pipe that is made up of 58% nickel, 20% chromium, carbon, manganese, silicon, iron, sulfur, aluminum and titanium in the composition. The pipes are highly corrosion resistant.
Inconel 625 pipe has very high fatigue strength, is nonmagnetic, and offers an operational temperature range from cryogenic to 2,000°F (1,093°C). Good oxidation resistance, exceptional fatigue strength, and good resistance to many corrosives.The material has 517MPa minimum yield strength and 930MPa minimum tensile strength.
Characteristics
- High creep-rupture strength
- Oxidation resistant to 1800° F
- Seawater pitting and crevice corrosion resistant
- Immune to chloride ion stress corrosion cracking
- Non-magnetic
We keep a selection of common sizes of Inconel 625 pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us request a quote.
Specification
|
Type |
Cold Drawn / Welded / ERW |
|
Outer Diameter Size |
Seamless - 1/4" NB to 6" NB (Nominal Bore Size) |
|
Wall Thickness |
Schedule 10 to Schedule 160 |
|
Length |
5 to 7 Meters, 09 to 13 Meters, Single Random Length, Double Random Length And Customize Size. |
|
Ends |
Plain Ends / Beveled Ends |
|
Delivery Conditions |
As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
|
Coating |
Electropolish, Mechanical Polish, Satin Finish, Passivated |
|
Other Testing |
NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc. |
|
Dimension |
All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME |
|
Value Added Services |
Draw / Expansion / Machining / Sand Blasting / Shot Blasting / Heat Treatment |
|
Packaging |
Loose / Bundle / Wooden Pallet / Wooden box-a / Plastic Cloth Wraps / Plastic End Caps / Beveled Protector |
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
60 |
|
Chromium, Cr |
22 |
|
Molybdenum, Mo |
9 |
|
Iron, Fe |
4 |
|
Niobium, Nb |
3.5 |
|
Titanium, Ti |
0.3 |
|
Manganese, Mn |
0.3 |
|
Aluminum, Al |
0.3 |
|
Silicon, Si |
0.25 |
|
Carbon, C |
0.05 |
|
Sulfur, S |
0.003 |
|
Phosphorous, P |
0.01 |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Hardness, Rockwell B (typical annealed) |
95 |
95 |
|
Tensile strength (for flat products (<4" thickness) and seamless tube and pipe) |
≥827MPa |
≥120000 psi |
|
Yield strength (for flat products (<4" thickness) and seamless tube and pipe) |
≥414MPa |
≥ 60000 psi |
|
Elongation at break (typical annealed) |
45% |
45% |
Application
The Inconel 625 Pipes and Tubes is used in the following applications:
- Aircraft ducting systems
- Aerospace
- Jet engine exhaust systems
- Engine thrust-reverser systems
- Specialized seawater equipment
- Chemical process equipment
Hot Tags: Inconel 625, Alloy 625, Nickel Pipe, UNS N06625, solid-solution strengthened nickel pipe, corrosion-resistant pipe, high-temperature pipe