• Ti-13Nb-13Zr Titanium Alloy(ASTM F1713)

    Lork Group specializes in supplying medical-grade ASTM F1713 Ti-13Nb-13Zr titanium alloy. Ti13Nb13Zr is a vanadium-free BETA titanium alloy developed in the 1990s for use in implants. It has a low

  • Commercially Pure Titanium Grade 2 (TA2)

    Grade 2 (TA2) Titanium is a versatile material offering an exceptional balance of strength, weight savings, and corrosion resistance. Its adaptability in welding, machining, and heat treatment makes

  • AMS 5876 / UNS R30003 / Elgiloy Material

    Lork Group is a trusted supplier of high-performance Elgiloy Alloy (AMS 5876 / UNS R30003), providing premium-quality cobalt-chromium-nickel-molybdenum strips, wires, and precision components. Our

  • UNS K93120 / AMS 6514 Maraging 300 Steel

    Maraging 300 (18Ni300 / UNS K93120) is an ultra-low-carbon nickel-cobalt-molybdenum-titanium maraging steel available in various forms—such as bars, plates, tubes, and strips—and complies with the

  • Nitronic 40 Round Bar(AMS 5656 / AMS 5595)

    Lork Group is a trusted supplier of high-quality Nitronic 40 (AMS 5656 / AMS 5595) round bar, providing premium austenitic stainless steel for aerospace, chemical processing, and cryogenic

  • AMS 5598 / Inconel X750 Nickel Alloy Strip

    Inconel X750 (AMS 5598) nickel alloy strip is a nickel-chromium alloy X750 for aerospace, nuclear, and industrial applications. Request a free quote today!

  • Ti-12Mo-6Zr-2Fe Titanium Alloy(ASTM F1813)

    Ti-12Mo-6Zr-2Fe (ASTM F1813) is a medical-grade β-type titanium alloy with exceptional performance. Its combination of non-toxicity, low modulus, high strength, and good toughness makes it an ideal

  • UNS K93540 / AMS 6515 Maraging 350(18Ni350)

    Maraging 350 (18Ni350 / UNS K93540 / AMS 6515) is the highest-strength grade in the 18Ni maraging steel series; it complies with the AMS 6515 standard and is available in various product forms,

  • Ti-15Mo Titanium Alloy (UNS R58210 , ASTM F2066)

    We specialize in supplying top-grade Ti-15Mo Titanium Alloy, a high-performance material known for its exceptional corrosion resistance, biocompatibility, and strength-to-weight ratio. Ideal for

  • Titanium 15-3-3-3 Alloy Strip (Ti-15V,UNS R58153)

    The customer base for Ti-15-3-3-3 is primarily concentrated in the fields of aerospace structural components, high-end fasteners, medical devices, and high-performance sports equipment.

  • 17-7PH Stainless Steel Bar (UNS S17700, AMS 5644)

    17-7 PH AMS 5644 is a semi-austenitic precipitation-hardening stainless steel that provides good corrosion resistance, good formability, and high strength.

  • 17-4 PH Round Stainless Steel Bar(UNS S17400 / AMS 5622)

    17-4PH stainless steel is a versatile engineering material that can achieve high strength through simple heat treatment, while also offering good corrosion resistance and ease of processing.