Ti-13Nb-13Zr Titanium Alloy(ASTM F1713)

Ti-13Nb-13Zr Titanium Alloy(ASTM F1713)

Lork Group specializes in supplying medical-grade ASTM F1713 Ti-13Nb-13Zr titanium alloy. Ti13Nb13Zr is a vanadium-free BETA titanium alloy developed in the 1990s for use in implants. It has a low elastic modulus, high mechanical properties, and excellent biocompatibility.
Send Inquiry

Welcome to Lork Group, your specialty metals manufacturer and exporter.

 

Ti-13Nb-13Zr is a near-β titanium alloy. The rods produced by Lork Group conform to ASTM F1713. This material is primarily used in medical implants, such as orthopedic implants, spinal fixation systems, and joint replacement components, among other modern medical applications.

 

Titanium Grade:Ti-13Nb-13Zr,UNS R58130

Standard: ASTM F1713

Size:

Diameter 1-300mm , customizable

Length 50mm-6000mm , customizable

Surface:Bright,Polished,Machined

MOQ:5KG (sample),100KG(Customization)

Packing method: Wooden box, PVC tube, carton

 

ASTM F1713 Ti-13Nb-13Zr Titanium Alloy parameters

 

ASTM F1713 Ti-13Nb-13Zr Titanium Alloy Custom

Lork Group is rooted in "Global Craftsmanship, Intelligent Manufacturing in China," with full-process quality control as the core, and rigorously selected suppliers. We professionally craft titanium alloys for you!.
Ti-13Nb-13Zr ASTM F1713 Titanium alloy bar

Ti-13Nb-13Zr Bar

Specifications

UNS R58130
ASTM F1713
Ti-13Nb-13Zr ASTM F1713 Titanium alloy sheet

Ti-13Nb-13Zr Plate

Specifications

UNS N09901
ISO 5832
Ti-13Nb-13Zr ASTM F1713 Titanium alloy tube

Ti-13Nb-13Zr Pipe

Specifications

UNS N09901
TC26
Ti-13Nb-13Zr ASTM F1713 Titanium alloy strip

Ti-13Nb-13Zr Strip

Specifications

UNS N09901
GB/T 13810

 

Advantages of ASTM F1713 Ti-13Nb-13Zr Titanium Alloy

      High-Purity Biomaterials:
      Ti-13Nb-13Zr was developed to address the toxicity issues associated with traditional titanium alloys, such as Ti-6Al-4V. This material's chemical composition eliminates impurities such as aluminum and vanadium, which are key contributors to neurotoxicity and cytotoxicity.

      Excellent Elastic Modulus:

     The elastic modulus of Ti-13Nb-13Zr titanium alloy is closest to that of human bone, which helps avoid implantable "stress shielding" and is more suitable for long-term implantation.

     The better ASTM F1713 Ti-13Nb-13Zr Titanium Alloy must be heat treated and conditioned.
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

titanium alloy

ASTM F1713 Ti-13Nb-13Zr Titanium Alloy Chemical Composition

Weight% Alloy 901
Ni -
Cr 12.5
Zirconium (Zr) 12.5 - 14.5%
Niobium (Nb) 12.5 - 14.5%
Co -
Cu -
Mn/Si/Al/C/S Trace
Titanium (Ti) Bal

ASTM F1713 Ti-13Nb-13Zr Titanium Alloy Mechanical Properties

Material Alloy 901
Tensile Strength  ≥ 900 MPa
Yield Strength  ≥ 800 MPa
Reduction of Area % ≥ 10%
Elastic Modulus 55 - 90 GPa

 For more ASTM F1713 Ti-13Nb-13Zr Titanium Alloy details, please contact us!

 

Contact now

 

 

 

 

 

Lork Group Company Introduction

 

Hot Tags: Ti-13Nb-13Zr Bar,Ti-13Nb-13Zr Titanium Alloy,UNS R58130,ASTM F1713,Near-β Titanium Alloy,β Titanium Alloy,Ti-13Nb-13Zr Titanium Alloy supplier

Send Inquiry