Haynes 263 Nickel Alloy Sheet
Haynes 263 Nickel Alloy Sheet Description
Haynes 263 (UNS N07263 / W.Nr. 2.4650) is an age-hardenable nickel-cobalt-chromium-molybdenum alloy sheet specifically designed to combine good age-hardened strength with excellent fabricability in the annealed condition. It is primarily intended to address the strain-age cracking issues commonly associated with γ′-strengthened alloys like Waspaloy and R-41, while maintaining ease of forming and welding.
Procurement Considerations
Confirm Standards and Product Form
Standard Specification: Clearly define the applicable standard for the material.
Form Distinction: Clearly specify whether the material is required as sheet or plate.
Clarify Delivery Condition
Default Condition: Typically delivered in the solution heat-treated condition to facilitate subsequent forming and welding by the customer.
Aged Condition: If specific strength levels are required for immediate use, confirm whether the supplier offers the material in an aged condition (a typical aging treatment is 800°C for 8 hours, followed by air cooling)
Supplier Qualification Verification
Melting Process: Require the supplier to specify the melting process (e.g., VIM+ESR/VAR) to ensure material purity.
Quality Documentation: Request the MTC (Material Test Certificate); if necessary, ask for third-party inspection reports or high-temperature creep-rupture performance data

Specification Reference
Thickness 0.5 – 100 mm (customizable)
Width Customizable
Surface BA / 2B / No. 1 / Brushed / Mirror, etc.
Haynes 263 Nickel Alloy Sheet Manufacturing and Pricing Reference
Haynes 263 Nickel Alloy Sheet
Annealing:
Annealing of this material can be performed at 1148°C (2100°F) and then rapidly air cooled or water quenched.
Hot Working:
Haynes 263 can be hot worked in the range of 1148-954°C (2100-1750°F).
The approximate prices offered by Lork Group are:
1. Stock Material: $40-60/kg (MOQ 50kg), $30-40/kg (300- 500 kg)
2. Custom Material - Metallurgy, heat treatment, and other solutions available (Price based on your requirements)
For more information, please contact:
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488

The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information!
Chemical Composition
| Weight% | Haynes 263 |
| Mn | ≤ 0.60 |
| Cr | 19.0 - 21.0 |
| Mo | 5.6 - 6.1 |
| Ti | 1.9 - 2.4 |
| Fe | ≤ 0.70 |
| Co | 19.0 - 21.0 |
| B/Si/Al/C/S | Trace |
| Ni | Bal |
Mechanical Properties
| Material | Haynes 263 |
| Tensile Strength | ≥ 940 MPa |
| Yield Strength | ≥ 550 MPa |
| Reduction of Area % | ≥ 39% |
| Melting Range |
1300 - 1355 °C |