AISI 316 Bar

AISI 316 Bar

Stainless Steel 316 Round Bar is made up of a stainless steel that is austenitic. The material has chromium, nickel and molybdenum in its composition.
Send Inquiry
AISI 316 Stainless Steel Bars & Rods – Premium Corrosion-Resistant Solutions by Lork Group

Lork Group is a trusted global supplier and manufacturer of high-quality AISI 316 stainless steel bars and rods, offering exceptional corrosion resistance, durability, and cost efficiency. As an austenitic stainless steel alloy, AISI 316 contains chromium (16-18%), nickel (10-14%), and molybdenum (2-3%), significantly enhancing its resistance to harsh environments compared to standard 304-grade stainless steel.

Enhanced Corrosion Resistance

– Molybdenum content provides superior resistance to chlorides, saltwater, and acidic environments.

Excellent Weldability & Formability

– Suitable for fabrication in construction, marine, and chemical industries.

Low Carbon Content (0.08% max)

– Reduces carbide precipitation, improving weldability and corrosion resistance.

Non-Magnetic & Hygienic

– Ideal for food processing, pharmaceuticals, and medical applications.

High Strength & Durability

– Maintains structural integrity in extreme conditions.

 

 

 

Specification

 

Dimensions

EN, DIN, JIS, ASTM, BS, ASME, AISI

Hex Bars in Milimeter

18mm – 57mm (11/16″ to 2-3/4″)

Round Bars Diameter

Outside Diameter in the range of 4mm to 500mm

Bright Bars Diameter

Outside Diameter in the range of 4mm to 100mm

Square Bars in Milimeter

18mm – 47mm (11/16″ to 1-3/4″)

Finish

Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Length

1 to 6 Meters, Custom Cut Lengths

Flat Bars in Milimeter

1/2" to 10" in thickness range of 2mm to 150mm,

Form

Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc.

Dimensions

EN, DIN, JIS, ASTM, BS, ASME, AISI

 

Chemical Composition

 

Element

Weight%

C

0.3 max

Mn

2.0 max

Si

0.75 max

P

0.045 max

S

0.030 max

Cr

16 - 18

Ni

10-14

Mo

2-3

Fe

67.845 min

 

Mechanical Properties

 

Density

8.0 g/cm³

Melting Point

1454 °C (2650 °F)

Tensile Strength

Psi – 75000 , MPa – 515

Yield Strength (0.2%Offset)

Psi – 30000 , MPa – 205

Elongation

40 %

 

Applications of AISI 316 Stainless Steel Bars

 

Due to its exceptional corrosion resistance and mechanical properties, AISI 316 bars are widely used in:

Marine & Offshore Engineering

  • Shipbuilding components, offshore platforms, and desalination plants.
  • Resistant to saltwater corrosion, making it ideal for coastal structures.

Chemical & Petrochemical Industry

  • Piping, valves, and reactors exposed to sulfuric acid, hydrochloric acid, and other aggressive chemicals.
  • Storage tanks and pressure vessels in corrosive environments.

Food & Pharmaceutical Processing

  • Equipment for brewing, dairy, and food packaging (non-reactive and easy to sterilize).
  • Pharmaceutical machinery requiring hygienic and corrosion-resistant materials.

Architectural & Construction Applications

  • Structural beams, fasteners, and reinforcement in corrosive environments.
  • Decorative and functional elements in coastal and urban infrastructure.

 

Why Choose Lork Group for AISI 316 Bars?

 

  • High-Quality Material Compliance – Meets ASTM A276, ASTM A479, and EN 10088-3 standards.
  • Precision Manufacturing – Available in round, square, hex, and flat bars with customized sizes.
  • Strict Quality Control – Rigorous testing ensures superior mechanical and chemical properties.
  • Competitive Pricing & Fast Delivery – Global supply chain with reliable stock availability.

 

AISI 316 stainless steel bars from Lork Group provide an optimal balance of corrosion resistance, strength, and cost-effectiveness, making them ideal for demanding industrial applications. Whether for marine, chemical, food processing, or construction, our AISI 316 bars deliver long-lasting performance.

 

Contact us today for specifications, pricing, and bulk orders!

 

Contact now

 

 

Surface Treatment

 

product-1200-750

 

Manufacturing Process

 

product-1200-682

 

Main Applications

 

product-1200-833

 

Packaging & Shipping

 

product-1200-690

product-1200-1147

 

FAQS

 

If you have any other questions, please contact me!

 

Q: Can you produce nickel alloy bars?

A: Yes, we can produce nickel alloy bars according to your requirements.

Q: What is your minimum order quantity?

A: Our minimum order quantity is 50 kg. Larger quantity, lower price.

Q: How long is your delivery time?

A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.

Q: Can you provide samples?

A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.

Q: How can l quickly get the price list?

A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.

Q: How do you control product quality?

A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.

Q: Can you provide processing services?

A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.

 

Hot Tags: aisi 316 bar, China aisi 316 bar manufacturers, factory

Send Inquiry