Monel 400 Pipe
Lork Group is a trusted global supplier and exporter of high-performance Monel 400 pipes and tubes, engineered for extreme durability and unmatched corrosion resistance in demanding industrial and marine environments.
Outstanding Corrosion Resistance
Seawater & Marine Applications – Resists saltwater corrosion, fouling, and pitting
High-Temperature Steam & Brackish Water – Ideal for desalination and offshore systems
Hydrochloric & Hydrofluoric Acids (De-aerated) – Superior performance in harsh chemical environments
Chloride Stress Corrosion Cracking (SCC) Resistance – Reliable in chloride-rich conditions
Alkalis & Neutral Salts – Excellent stability in alkaline solutions
We keep a selection of common sizes of Monel 400 Pipe in stock. If you have high requirements for the delivery time of the pipe and tubes, you can confirm with us request a quote.
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
Remainder |
|
Copper, Cu |
28-34 |
|
Iron, Fe |
2.5 max |
|
Manganese, Mn |
2 max |
|
Silicon, Si |
0.5 max |
|
Carbon, C |
0.3 max |
|
Sulphur, S |
0.024 |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile strength(annealed) |
517-620 MPa |
75-90 ksi |
|
Yield strength |
172-345 MPa |
25-50 ksi |
|
Modulus of elasticity |
179 GPa |
26000 ksi |
|
Poisson's ratio |
0.32 |
0.32 |
Application
Marine & Offshore Engineering – Seawater piping, pump shafts, heat exchangers
Oil & Gas Industry – Downhole components, valves, and fittings
Chemical Processing – Acid-handling equipment, evaporators
Power Generation – Condenser tubes, boiler feedwater systems
Aerospace & Defense – Hydraulic lines, fuel delivery systems
Lork Group's Supply Advantage
Wide Stock Availability – Ready-to-ship common sizes for fast delivery
Custom Manufacturing – Precision-cut pipes & tubes to your specifications
Global Export Expertise – Reliable logistics for seamless procurement
Request a Quote Today! – Get high-quality Monel 400 pipes & tubes with competitive lead times.
Hot Tags: Monel 400 alloy Supplier,Monel 400 Pipe,UNS N04400,ASTM B165 Seamless pipe,ASTM B725 Welded pipe
You Might Also Like
Send Inquiry