AMS 5659 15-5PH/XM-12(UNS S15500)
Products Description

15-5PH stainless steel Bars & Wire and Forging ring(UNS S15500) conform to the aerospace materials specification AMS 5659. Also known as XM-12 or PH15-5, 15-5PH is a martensitic precipitation-hardening stainless steel designed to combine high strength, good corrosion resistance, and excellent toughness. It is a niobium (Nb)-containing chromium-nickel-copper alloy whose mechanical properties are achieved through controlled solution heat treatment and subsequent precipitation aging.
The AMS 5659 specification specifically covers corrosion-resistant steel bars, wires, forgings, flash-welded rings, and extrusions. This material is designed for aerospace and other engineering applications with extremely high mechanical performance requirements, particularly for large cross-sections and transverse applications.
Precipitation hardening achieves high strength, and its mechanical properties can be tuned through different aging treatments, including H900, H925, H1025, H1075, H1100, and H1150. Compared to traditional 17-4PH stainless steel, 15-5PH stainless steel has superior transverse toughness and ductility, making it suitable for critical structural components and precision engineering parts.
Supply profiles and delivery status
This beacon covers corrosion-resistant steel in bar, wire, forging, flash welded ring, and extrusion form under solution heat treatment conditions, with a nominal diameter, thickness, or hexagon of 12 inches (305 mm) or less, minimum distance between parallel sides, maximum cross-sectional area of 144 square inches (930 square centimeters), and any size of steel for forging, flash welded ring, or extrusion.
Typically delivered in Condition A (solution-treated state), the required strength, hardness, and toughness are subsequently achieved through precipitation aging. Depending on the application requirements, different conditions such as H900, H925, H1025, H1075, H1100, and H1150 can be obtained by adjusting the aging temperature and holding time at 15-5PH. Generally, lower-temperature aging yields higher strength and hardness, while higher-temperature aging improves ductility and toughness.
Minimum tensile properties, SI units
|
Condition
|
Specimen Orientation
|
Tensile Strength
MPa
|
Yield Strength at 0.2% Offset
MPa
|
Elongation in 50 mm or 4D
%
|
Reduction of Area
%
|
|
H900
|
Longitudinal
Transverse
|
1310 1310 |
1172 1172 |
10 6 |
35 20 |
| H925 |
Longitudinal
Transverse
|
1172 1172 |
1069 1069 |
10 7 |
38 25 |
| H1025 |
Longitudinal
Transverse
|
1069 1069 |
1000 1000 |
12 8 |
45 32 |
| H1075 |
Longitudinal
Transverse
|
1000 1000 |
862 862 |
13 9 |
45 33 |
| H1100 |
Longitudinal
Transverse
|
965 965 |
793 793 |
14 10 |
45 34 |
| H1150 |
Longitudinal
Transverse
|
931 931 |
724 724 |
16 11 |
50 35 |
chemical composition
| Element | min | max |
| C | -- | 0.07 |
| Mn | -- | 1.00 |
| Si | -- | 1.00 |
| P | -- | 0.030 |
| S | -- | 0.015 |
| Cr | 14.00 | 15.50 |
| Ni | 3.50 | 5.50 |
|
Nb |
5xC | 0.45 |
| Cu | 2.50 | 4.50 |
| Mo | -- | 0.50 |
15-5PH vs. 17-4PH Stainless Steel
Both 15-5PH and 17-4PH are martensitic precipitation-hardening stainless steels, possessing high strength and good corrosion resistance. However, 15-5PH was developed to improve the transverse toughness and ductility of the traditional 17-4PH.
The main difference between the two lies in their microstructure and mechanical properties. 15-5PH typically exhibits better transverse toughness and greater stability at large cross-sections, making it suitable for demanding structural applications.
Which One Should You Choose?
17-4PH is a versatile precipitation-hardening stainless steel suitable for applications requiring high strength and good corrosion resistance. However, when components require improved transverse toughness, better ductility, and more consistent properties in larger cross-sections, 15-5PH offers a distinct advantage.
If you would like a more detailed comparison of the two and information about 17-4PH, you can click on the image or the blue underlined link to jump to the product page, making it easier for you to compare and choose the better solution.
For aerospace and other demanding structural applications, 15-5PH stainless steel manufactured to AMS 5659 provides a reliable material option where strength and transverse mechanical performance must be considered together.
Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488
Hot Tags: 15-5PH Stainless Steel, AMS 5659, UNS S15500, XM-12,15-5PH,15-5PH Aerospace Stainless Steel,15-5PH vs 17-4PH Stainless Steel,15-5PH Precipitation Hardening Stainless Steel
You Might Also Like