AISI 304 Stainless Steel Bar (UNS S30400)

AISI 304 Stainless Steel Bar (UNS S30400)

AISI 304 has corrosion resistance and strength properties. The material is strong with 515MPa minimum tensile strength and 205MPa minimum yield strength. It also can operate under high temperatures.
Send Inquiry

Lork Group is a trusted professional stainless steel supplier and exporter, specializing in high-quality AISI 304 bars & rods that deliver exceptional cost-performance efficiency. Our products are manufactured under strict quality control to meet international standards, ensuring durability, strength, and superior corrosion resistance for diverse industrial applications.

 

AISI 304 Stainless Steel Bar – Composition & Key Properties

 

AISI 304 is an austenitic stainless steel composed of 18% chromium and 8% nickel, making it highly resistant to corrosion and oxidation. Its excellent mechanical properties include:

High Tensile Strength: Minimum 515 MPa

Yield Strength: Minimum 205 MPa

Hardness: 58-60 HRC (excellent machinability)

High-Temperature Resistance: Performs well in elevated temperatures

Corrosion Resistance: Resists rust in freshwater, marine, and chemical environments

These properties make AISI 304 bars ideal for demanding applications where strength, durability, and resistance to harsh conditions are critical.

 

Chemical Composition

 

Element

Weight%

C

0.08 max

Mn

2.0 max

Si

0.75 max

P

0.045 max

S

0.030 max

Cr

18.0 - 20.0

Ni

8-11

Mo

-

 

Mechanical Properties

 

Density

8.0 g/cm³

Melting Point

1400 °C (2550 °F)

Tensile Strength

Psi – 75000 , MPa – 515

Yield Strength (0.2%Offset)

Psi – 30000 , MPa – 205

Elongation

35 %

 

Key Applications of AISI 304 Stainless Steel Bars

 

1. Construction & Architecture

Used in structural supports, reinforcements, and frameworks

Ideal for bridges, buildings, and architectural elements due to high strength

2. Marine Industry

Saltwater corrosion resistance makes it perfect for shipbuilding, docks, and offshore structures

3. Automotive Sector

Used in shafts, axles, and high-stress components due to wear resistance

4. Industrial Machinery

Suitable for heavy-duty equipment operating under high pressure and temperature

5. Food Processing & Medical Devices

Hygienic, non-reactive surface for food-grade equipment

Used in surgical instruments & medical tools due to sterilization ease

6. Chemical Processing

Resists corrosive chemicals, making it ideal for tanks, valves, and piping systems

 

Why Choose Lork Group as Your AISI 304 Supplier?

 

As a leading stainless steel supplier in China, we ensure:

  • High-quality AISI 304 bars with strict quality control
  • Competitive pricing & cost-performance efficiency
  • Custom sizes & specifications available
  • Reliable global export services

 

Whether you need AISI 304 round bars, rods, or custom-cut stainless steel products, Lork Group delivers durable, high-performance solutions tailored to your industry needs.

 

Contact Us Today for Premium Stainless Steel Solutions!

Upgrade your projects with high-grade AISI 304 stainless steel bars – strong, corrosion-resistant, and built to last.

 

Contact now

 

 

Hot Tags: AISI 304, Stainless Steel Bar, 304 Round Bar, UNS S30400, austenitic stainless bar, corrosion-resistant bar, non-magnetic bar, cold-finished bar

Send Inquiry