Incoloy 800 Nickel Alloy Bar (UNS N08800)
Lork Group as a professional trustworthy Incoloy alloy supplier and exporter, we produce Incoloy 800 round bars & rods with high cost performance.
Incoloy 800 which has high electrical and thermal conductivity. These properties and its chemical composition make Alloy 800 Round Bars fabricable and highly resistant to corrosive environments.
As a leading Incoloy 800 supplier in China, our products pass strict quality control and testing and ensure that the products meet standards and customer requirements. Lork Group manufactures and produces bars of various sizes.Contact us as your Alloy 800 Stock Distributor and Supplier.
Click to contact the sales team
Email: [susan@lorkgroup.com]
WhatsApp: [+ 86 199 37075488]
Specification
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Wire |
Thickness starting from 0.05mm |
|
Round bar size |
Diameter: 3-~800mm |
|
Hex Bar size |
2-100mm A/F |
|
Flat bar size |
Thickness: 2 -100mm / Width: 10 to 500mm |
|
Square bar size |
4 to 100mm |
|
Rectangular Bars Size |
33 x 30mm to 295 x 1066mm |
|
Hollow Bar |
32mm OD x 16mm ID to 250mm OD x 200mm ID |
|
Tolerance |
H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements |
|
Finish |
Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
Chemical Composition
|
Elements |
Content (%) |
|
S |
≤0.015% |
|
C |
≤0.10% |
|
AI |
0.15%~0.60% |
|
Cu |
≤ 0.75% |
|
Ni |
30.0%~35.0% |
|
Si |
≤1.00% |
|
Fe |
≥39.5% |
|
Mn |
≤1.50% |
|
Ti |
0.15%~0.60% |
Mechanical Composition
|
Condition & Size |
Tensile Strength |
Yield Strength |
Elongation |
Reduction of Area |
Hardness |
|
MPa, min |
MPa, min |
%, min |
%, min |
Rockwell, max |
|
|
Hot worked, as-hot-worked |
550 |
240 |
25 |
... |
... |
|
Cold-worked and hot-worked, annealed |
515 |
205 |
30 |
... |
... |
|
Condition & Size |
Tensile Strength |
Yield Strength |
Elongation |
Reduction of Area |
Hardness |
|
MPa, min |
MPa, min |
%, min |
%, min |
Rockwell, max |
|
|
Hot worked, as-hot-worked |
550 |
240 |
25 |
... |
... |
|
Cold-worked and hot-worked, annealed |
515 |
205 |
30 |
... |
... |
|
Condition & Size |
Tensile Strength |
Yield Strength |
Elongation |
Reduction of Area |
Hardness |
Applications
Incoloy 800 Round Bars is used heavily in the chemical and electronics industries. Inconel 800 Flat Bars is used in viscose rayon and polymer production, food processing, reactors, tubes, aerospace engineering, military and other applications. In application temperatures above 300 Degree C (572 Degree F), alloy 800 Square Bars stands out for a low carbon concentration.
Incoloy 800 Threaded Bars is also used in structural applicatio sistance to corrosion is a prime consideration. alloy 800 Hollow Bars is frequently dual certified as a result of processing which provides the strength of 200 with the stability of the compositional controls. Because of this, Inconel 800 Hexagonal Bars can lend themselves well to slightly different purposes.