Nimonic 90 Nickel Alloy Bar

Nimonic 90 Nickel Alloy Bar

Nimonic 90 rod (UNS N07090). Suitable for turbine blades, fasteners, and springs operating at temperatures up to 870°C. Common specifications: diameters ranging from Φ0.025 mm to 21 mm.Stock material: $70–$80/kg (MOQ: 50–100 kg)
Send Inquiry

 

Nimonic 90 Nickel Alloy Bar Description

 

Due to its exceptional high-temperature strength, outstanding creep and stress-rupture resistance, and excellent oxidation and corrosion resistance, Nimonic 90 nickel alloy is primarily used to manufacture critical components operating at high temperatures (815–870°C). Its core applications are in aerospace engines, though it is also utilized in high-end industrial sectors.

 

When purchasing Nimonic 90 alloy bars, Lork Group offers the following recommendations based on extensive supply experience:


1. Clarify Requirements and Standards:

Define your application environment (temperature, stress, and operating medium) and specific material performance requirements.

Ensure the material complies with relevant standards and clearly specify the required material condition and heat treatment process (e.g., solution treatment, aging treatment, spring temper, etc.).

 

2. Evaluate Production and Quality Inspection Capabilities:

Request a comprehensive Material Test Certificate (MTC) from the supplier to guarantee reliable quality. Third-party re-inspection may be necessary for critical applications. Lork Group offers services such as video-based technical consultations and customized production processes.

 

Please contact us if you are interested in Nimonic 90 nickel alloy bars.

 

 

Nimonic 90 Nickel Alloy Parameters

 

Cold-drawn/ground bars Approx. Φ0.025 mm – 21 mm High dimensional accuracy; suitable for machining or cold heading
Hot-rolled/forged bars Approx. Φ10 mm – 300 mm Large-diameter bars; commonly used for components such as turbine discs and blades

Customized dimensions: In addition to standard stock sizes, we offer custom cutting based on drawings and rolling or forging to specific diameters.

 

Nimonic 90 Nickel Alloy Bar Manufacturing and Pricing Reference

 

 

Nimonic 90 Nickel Alloy Bar

   

When processing Nimonic 90 alloy, special attention must be paid to its material properties, particularly regarding heat treatment and welding requirements:

Welding Performance:

The alloy exhibits excellent welding characteristics and can be welded using methods such as Tungsten Inert Gas (TIG) welding.

Reference prices provided by Lork Group are as follows:
1. Stock material: $70–$80/kg (MOQ: 50–100 kg); $50–$60/kg (300–500 kg)
2. Processing services: Cutting, machining, milling, etc. (pricing depends on material loss and processing method)
3. Customized materials: Metallurgical, heat treatment, and other solutions available (pricing depends on specific requirements)
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

Nimonic 90 Nickel Alloy rod

 

 The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information! 

 

 

Nimonic 90 Nickel Alloy Chemical Composition

 

Weight% Nimonic 90
Mn ≤ 0.40
Cr 18.0 - 21.0
Mo 26.0 - 30.0
Ti 2.0 - 3.0
Ai 1.0 - 2.0
Co 15.0 - 21.0
Si/Fe/C/S Trace
Ni Bal

 

 

Nimonic 90 Nickel Alloy Mechanical Properties

 

Material Extruded Bar: Nimonic 90 bar Precipitation Treated (BS HR2)

Material Nimonic 90
Tensile Strength 1080 min
Yield Strength 695 min
Elongation (%) 20 min
Hardness HV 310 min

 For more Nimonic 90 Nickel Alloy details, please contact us!

 