Inconel 738LC Nickel Alloy Bar (UNS R30783)

Inconel 738LC Nickel Alloy Bar (UNS R30783)

Inconel 738LC is a nickel-based precipitation-hardening superalloy with a typical material density of 7.81 g/cm³. ‘LC’ refers to low carbon, a property that gives it excellent resistance to oxidation and creep at high temperatures.
Send Inquiry

 

W.Nr.2.4880 Haynes HR 160 Nickel Alloy Description

 

Inconel 738LC Nickel Alloy Bar is a difficult-to-machine material. Due to its excellent high-temperature performance, Inconel 738LC is widely used in the manufacture of key hot-end components such as turbine blades, combustion chambers, and fasteners in aircraft engines.

 

Purchasing Recommendations Inconel 738LC Nickel Alloy Bar:


1. Clarify Requirements:

First, confirm your application's specific requirements for high-temperature strength, corrosion resistance, creep life, and maximum operating temperature.

 

2. Verify Materials:

Require suppliers to provide detailed material certification documentation to ensure that the chemical composition and mechanical properties comply with relevant standards or technical protocols.

 

3.Focus on Process:

For critical components, prioritize materials produced using advanced processes such as vacuum induction melting and electroslag remelting to ensure high purity and microstructure uniformity.

 

If you are interested in Inconel 738LC Nickel Alloy Bar, please click the circle icon below to initiate an online communication.

 

Inconel 738LC Nickel Alloy Manufacturing And Pricing Reference

 

   Weldability:

   Weldability is poor and requires high process requirements. Specialized methods such as TIG are required, along with carefully controlled heat input. Preheating and post-heat treatment are often necessary to prevent cracking.

   Heat Treatment:

   Performance depends on a precise heat treatment schedule, typically consisting of solution treatment and aging. For example, an optimized heat treatment schedule might include solution treatment (1230°C for 2 hours, furnace cooling) followed by an intermediate heat treatment (1120°C for 2 hours, furnace cooling) and an aging treatment (900°C for 24 hours, air cooling).

     Lork Group offers customized Inconel 738LC Nickel Alloy Bar.The approximate prices offered by Lork Group are:
1. Stock Material: $25-30/kg (MOQ 50kg), $20-25/kg (200-500kg)
2. Processing: Cutting, chipping, milling, etc. (Price based on material loss and processing method)
For more information, please contact:

 Email: susan@lorkgroup.com
 WhatsApp: +86 19937075488

Inconel 738LC Nickel Alloy

 

 The above prices are average market prices for materials and are for reference only. For real-time pricing, please send us your order request for more information! 

 

 

Inconel 738LC Nickel Alloy Chemical Composition

 

Weight% Inconel 738LC
Co 8-9
Cr 15.7-16.3
Mo 1.5 - 2.0
W 2.4-2.8
Ta 1.4 - 2.0
Al+Ti 6.5
Cb/Si/Al/C/S Trace
Ni Bal

 

 

Inconel 738LC Nickel Alloy Mechanical Properties

 

 

Material Inconel 738LC
Tensile Strength 690
Yield Strength 895
Reduction of Area % ≥5%
Sectional Shrinkage ≥10%

 For more Inconel 738LC Nickel Alloy details, please contact us!

 

Contact now

Hot Tags: Inconel 738LC, Alloy 738LC, Nickel Bar, AMS 5391, UNS R30783, ASTM B637, cast nickel superalloy, high temperature alloy bar, turbine blade material