Monel K500 Strip
When it comes to high-performance nickel-copper alloys, Monel K500 Strip stands out for its exceptional strength, corrosion resistance, and versatility. As a precipitation-hardenable alloy, Monel K500 combines the outstanding corrosion resistance of Monel 400 with enhanced mechanical properties, making it ideal for demanding industrial applications.
Why Choose Monel K500 Strip?
-
Superior Corrosion Resistance
Monel K500 Strip performs exceptionally well in marine environments, chemical processing, and sour-gas applications, resisting degradation from saltwater, acids, and alkalis.
-
High Strength & Hardness
Thanks to age-hardening treatments, Monel K500 Strip offers greater tensile strength and hardness compared to standard nickel-copper alloys.
-
Temperature Stability
It retains excellent mechanical properties from cryogenic temperatures up to 480°C (900°F), making it suitable for extreme conditions.
-
Non-Magnetic Properties
Ideal for applications requiring non-magnetic materials, such as marine and electronic components.
-
Fabrication Flexibility
Monel K500 Strip can be welded, machined, and formed using standard methods, though post-weld heat treatment is recommended for optimal performance.
Chemical Composition
|
Element |
Content (%) |
|
Nickel, Ni |
66 |
|
Copper, Cu |
29 |
|
Aluminum, Al |
2.7 |
|
Iron, Fe |
1 |
|
Manganese, Mn |
0.7 |
|
Tungsten, W |
0.6 |
|
Silicon, Si |
0.25 |
|
Carbon, C |
0.1 |
|
Sulfur, S |
0.01 |
Physical Properties
|
Properties |
Metric |
Imperial |
|
Density |
8.45 g/cm³ |
0.305 lb/in³ |
|
Melting point |
1338°C |
2440°F |
Mechanical Properties
|
Properties |
Metric |
Imperial |
|
Tensile strength |
1000 MPa |
145000 psi |
|
Yield strength (at strain 0.200%) |
655 MPa |
95000 psi |
|
Elongation at break |
22% |
22% |
|
Reduction of area |
40% |
40% |
|
Hardness, Rockwell C |
27 |
27 |
Applications of Monel K500 Strip
- Marine Engineering (pump shafts, propeller blades)
- Oil & Gas (valve components, drill collars)
- Chemical Processing (heat exchangers, reactor vessels)
- Aerospace & Defense (non-magnetic fasteners, precision parts)
As a trusted Monel K500 Strip supplier, Lork Group provides customized solutions tailored to your mechanical and dimensional requirements. Whether you need corrosion-resistant marine components or high-strength industrial parts, Monel K500 Strip delivers unmatched reliability.
For specialized specifications, consult with our experts to ensure your material meets exact performance standards. Choose Monel K500 Strip for durability, strength, and resistance in the harshest environments.
Hot Tags: Monel K500 alloy Supplier,Monel K500 sheet,ASTM B127,UNS N05500,alloy K500 strip