AMS 4911 Ti-6Al-4V Sheet
Ti-6Al-4V is a titanium alloy comprising 6% aluminum, 4% vanadium, and the remainder titanium. This composition balances strength, ductility, and corrosion resistance, making it the most widely used titanium alloy.
AMS 4911 is an Aerospace Material Specification governing the production and quality of Ti-6Al-4V (Grade 5 titanium alloy), primarily in sheet, strip, and plate forms. This standard ensures that the material meets stringent aerospace requirements for performance and safety.
AMS 4911 Ti-6Al-4V sheet are pivotal in industries prioritizing strength, weight, and corrosion resistance. Their use is governed by stringent standards, with ongoing advancements in forming techniques and applications in additive manufacturing complementing traditional rolled products.
Chemical Composition
|
Element |
Weight |
|
Aluminum |
5.5 – 6.75% |
|
Vanadium |
3.5 – 4.5% |
|
Iron |
0.30% max |
|
Oxygen |
0.20% max |
|
Carbon |
0.08% max |
|
Nitrogen |
0.05% max |
|
Hydrogen |
0.015% max |
|
Yttrium |
0.005% |
|
Titanium |
Balance |
|
Other Elements |
0.40% |
Mechanical Properties
|
0.2% Proof Stress |
Tensile Strength |
Elongation |
Reduction of area |
Hardness |
|
MPA |
MPA |
% |
% |
HRC |
|
Min |
Min |
Min |
Min |
|
|
830 |
900 |
8 |
20 |
36 |
Comparison with Other Standards
AMS 4928: This covers Ti-6Al-4V in bar, forging, and ring forms.
AMS 6931: Specifies beta-annealed Ti-6Al-4V with enhanced fracture toughness.
ASTM Standards: Less stringent than AMS, which prioritizes aerospace-critical properties.
Processing and Heat Treatment
Annealed Condition: AMS 4911 Ti-6Al-4V sheet typically specifies material supplied in the annealed state to relieve stresses and enhance ductility.
Fabrication: Guidelines for welding (e.g., inert gas shielding), machining, and forming to prevent contamination or embrittlement.
Application
Aerospace: Fuselage panels, wing components, engine parts (e.g., fan blades, compressor discs), and fasteners.
Other Industries: While AMS 4911 is aerospace-focused, Ti-6Al-4V is also used in the marine, chemical, and medical sectors (under different standards).
Manufacturing Process

Main Applications

Packaging & Shipping


FAQS
If you have any other questions, please contact me!
Q: Can you produce nickel alloy bars?
A: Yes, we can produce nickel alloy bars according to your requirements.
Q: What is your minimum order quantity?
A: Our minimum order quantity is 50 kg. Larger quantity, lower price.
Q: How long is your delivery time?
A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.
Q: Can you provide samples?
A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.
Q: How can l quickly get the price list?
A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.
Q: How do you control product quality?
A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.
Q: Can you provide processing services?
A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.
Hot Tags: ams 4911 ti-6al-4v sheet, China ams 4911 ti-6al-4v sheet manufacturers, factory
You Might Also Like
Send Inquiry