Haynes 233 Alloy Sheet
Haynes 233 is a new nickel-based superalloy designed to provide excellent oxidation resistance and superior creep strength at extreme temperatures up to 1149°C (2100°F).Haynes 233 Alloy Sheet
-
Haynes 214 Alloy Sheet(UNS N07214)
Haynes 214 Alloy (UNS N07214) is a nickel – chromium-aluminum-iron alloy, developed to provide the optimum in high-temperature oxidation resistance for a wrought austenitic material
-
Haynes 75 Alloy Sheet(UNS N06075)
Haynes 75 alloy sheet (UNS N06075) is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature
-
Nickel 201 Alloy Sheet
Nickel 201 alloy sheet has the same characteristics Nickel 200 but has lower carbon levels. These properties, and its chemical composition, make Nickel alloy 201 fabricatable and highly resistant to
-
Nickel 200 Alloy Sheet(UNS N02200, ASTM B162)
Nickel 200 has an 'absolute affinity' for alkalis, 'passivation immunity' to hydrogen fluoride, extremely low gas permeability, and 'non-magnetic' stability. Its ultra-high 'purity' means that its
-
Hastelloy N Alloy Sheet
Hastelloy N Alloy (UNS N10003) is a nickel-base alloy that was invented at Oak Ridge National Laboratories as a container material for molten fluoride salts. It has good oxidation resistance to hot
-
AISI 321 Sheet
Lork Group is one of the leading suppliers of stainless steel sheets, offering high-quality products at competitive prices. We maintain a large stock of AISI 321 sheet, plate, and strip, compliant
-
AISI 304L(UNS S30403,ASTM A240/A480)
Lork Group is one of the leading suppliers of stainless steel sheets, offering high-quality products at competitive prices. We maintain a large stock of AISI 304L sheet, plate and strip, compliant
-
AISI 304 Stainless Steel Sheet (UNS S30400)
Lork Group is AISI 304 sheet supplier and exporter. Premium stainless steel grade 304 is a very low carbon, austenitic chromium-nickel steel with good corrosion resistance.
-
AISI 316L Stainless Steel Sheet (UNS S31603)
AISI 316L sheet good corrosion resistance to most chemicals, salts, and acids and molybdenum content helps resistance to marine environments.
-
AISI 316 Stainless Steel Sheet (UNS S31600)
Lork Group is AISI 316 sheet supplier and exporter. The material is a higher-quality alloy added molybdenum and an increased chromium and nickel content, which means that has a higher resistance to
-
AISI 310S Stainless Steel Sheet (UNS S31008)
Lork Group is AISI 310S sheet supplier and exporter. The material is suitable for many common welding processes such as arc or TIG welding and can also be used for forging and cold forming.