AISI 316 Sheet

AISI 316 Sheet

Lork Group is AISI 316 sheet supplier and exporter. The material is a higher-quality alloy added molybdenum and an increased chromium and nickel content, which means that has a higher resistance to corrosion.
Send Inquiry

Lork Group is AISI 316 sheet supplier and exporter. The material is a higher-quality alloy added molybdenum and an increased chromium and nickel content, which means that has a higher resistance to corrosion.

 

The addition of molybdenum makes AISI 316 sheets more corrosion and oxidation-resistant and very suitable for applying for instance in areas near the sea or a slightly alkaline environment. In addition to these properties, this material is easy to process, form and weld.

 

The properties of AISI 316 sheets

 

  • Excellent resistance to various aggressive media
  • Heat resistance
  • Higher expansion rate
  • Higher stability, forexample when used in an environment with salty or acidic air.

 

We keep a selection of common sizes of AISI 316 sheet in stock. If you have high requirements for the delivery time of the plates, you can confirm with us request a quote.

 

Specification

 

Thickness

0.3mm~200mm

Width

1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length

2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Standard

JIS, AISI, ASTM, GB, DIN, EN, etc

Surface

the surface and finish of stainless steel 310s sheet:
2B, 2D, BA, NO.1, NO.4, NO.8, 8K, mirror, checkered, embossed, hair line, sand
blast, Brush, etching, etc

Package

Shrink-wrapped ,Carton boxes,Wooden pallets,Wooden boxes ,Wooden crates Etc.
required.

 

Chemical Composition

 

Elements

AISI 316

C

0.0-0.07

Mn

0.0-2.0

Si

0.0-1.0

P

0.0-0.05

S

0.0-0.02

Cr

16.50-18.50

Mo

2.00-2.50

Ni

10.00-13.00

Ti

-

Fe

balance

 

Mechanical Properties

 

Grade

AISI 316 Sheet (up to 8 mm thick)

AISI 316 Plate (8 - 75 mm thick)

Tensile Strength (MPa)

530 - 680

520 - 670

Proof Stress (MPa)

240 Min

220 Min

Elongation A50 mm

40 Min %

45 Min %

 

Application

 

Common uses of AISI 316 sheet include:

  • Boat Fittings
  • Brewery Equipment
  • Chemical Transportation Containers
  • Chemical & Petrochemical Equipment
  • Coastal Architectural Paneling
  • Coastal Balustrading
  • Food Processing Equipment
  • Heat Exchangers
  • Medical Implants
  • Mining Screens
  • Nuts & Bolts
  • Laboratory Benches & Equipment
  • Springs

 

Surface Treatment

 

product-1200-750

 

Manufacturing Process

 

product-1200-682

 

Main Applications

 

product-1200-833

 

Packaging & Shipping

 

product-1200-690

product-1200-1147

 

FAQS

 

If you have any other questions, please contact me!

 

Q: Can you produce nickel alloy bars?

A: Yes, we can produce nickel alloy bars according to your requirements.

Q: What is your minimum order quantity?

A: Our minimum order quantity is 50 kg. Larger quantity, lower price.

Q: How long is your delivery time?

A: Generally delivery time for stock is 3 days, and customization takes 15 working days or more, but it is also affected by your specific requirements or order quantity.

Q: Can you provide samples?

A: For small parts, we can provide free sample of regular sizes, but the shipping costs will be borne by you. For large parts sample, we will include it in the order amount. Please confirm with our sales department for your specific requirements.

Q: How can l quickly get the price list?

A: Directly send us email with detailed specification, and you will get the official price list in 1 hour.

Q: How do you control product quality?

A: From the selection of raw materials to transportation packaging, every production process will be testing and evaluated. Only products that have passed all tests can be delivered for export.

Q: Can you provide processing services?

A: Yes, we also provide processing services to our customers. It is one of our goals to provide specialized services such as bending, water cutting, laser cutting, digging holes, welding, slitting of coils, and other fabrications according to the drawings.

 

Hot Tags: aisi 316 sheet, China aisi 316 sheet manufacturers, factory

Send Inquiry