Haynes 230 Sheet(UNS N06230)
Haynes 230 Sheet is used for a wide variety of applications in the aerospace and power generation industries because of its excellent high-temperature strength, thermal stability, environmental
-
Incoloy 800ht Sheet
Incoloy 800HT are nickel-iron-chromium alloys with good strength and excellent resistance to oxidation and carburization in high-temperature exposure.
-
Incoloy 825 Sheet
Incoloy 825 Sheet is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. Alloy 825 chemical composition is designed to provide exceptional resistance to many corrosive
-
Monel K500 Sheet
Monel K500 sheet is made up of a nickel copper alloy that has 63% nickel and 28% copper minimum with carbon, manganese, silicon, sulfur and iron in the composition.
-
Inconel X750 Sheet (ISO 6208, AMS 5542, AMS 5598)
The processing and heat treatment of Inconel X750 must follow its temperament: the forming process must be soft (solution state), welding must be careful (to prevent strain aging cracks), and the
-
Inconel 718 Nickel Alloy Sheet (AMS 5596, UNS N07718)
Lork Group has ample stock of Inconel 718 alloy in various specifications, including rods, plates, tubes, coils, strips, and wires. We support custom processing and third-party testing, and have a
We're well-known as one of the leading nickel alloy sheet manufacturers in China. Please feel free to buy cheap nickel alloy sheet for sale here and get pricelist from our factory. For price consultation, contact us.
Send Inquiry