Incoloy 825 Nickel Alloy Sheet (UNS N08825)
In today's industrial landscape, materials that can withstand extreme corrosive environments while maintaining structural integrity are in high demand. Incoloy 825, a nickel-iron-chromium alloy enhanced with molybdenum, copper, and titanium, stands out as a premier choice for industries requiring exceptional corrosion resistance and durability. As a leading supplier and exporter of Incoloy 825 Sheet & Plate, Lork Group is committed to delivering precision-engineered solutions that meet the highest quality standards.
Why Choose Incoloy 825 Sheets & Plates?
Outstanding Corrosion Resistance
Resists pitting, crevice corrosion, and stress-corrosion cracking (SCC).
Performs exceptionally well in sulfuric acid, phosphoric acid, and seawater environments.
High-Temperature Stability
Maintains strength and oxidation resistance at elevated temperatures, making it suitable for heat exchangers and furnace components.
Versatile Industrial Applications
- Chemical Processing: Reactors, tanks, and piping systems handling corrosive chemicals.
- Oil & Gas: Downhole tubing, pipelines, and sour gas environments.
- Pollution Control: Scrubbers, flue gas desulfurization systems.
- Nuclear & Power Generation: Fuel reprocessing, acid production equipment.
Specification
|
Dimensions : |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Width: |
1000 MM TO 2500 MM |
|
Thick: |
0.5 MM TO 200 MM |
|
Length: |
100MM TO 600MM |
|
Form : |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange) |
|
Finish : |
Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated) |
|
Hardness : |
Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc. |
Chemical Composition
|
Element |
Content (%) |
|
Ni |
38.0-46.0 |
|
Fe |
22.0 min |
|
Cr |
19.5-23.5 |
|
Mb |
2.5-3.5 |
|
Cu |
1.5-3.0 |
|
Ti |
0.6-1.2 |
|
C |
0.05 max |
|
Mn |
1.0 max |
|
S |
0.03 max |
|
Si |
0.5 max |
|
AI |
0.2 max |
Tensile Properties
|
Form |
Condition |
0.2% Proof Stress |
Tensile Strength |
Elong |
|
Tube |
Annealed |
440 |
770 |
35 |
|
Tube |
Cold drawn |
880 |
1000 |
15 |
|
Bar |
Annealed |
325 |
690 |
45 |
|
Plate |
Annealed |
340 |
660 |
45 |
|
Sheet |
Annealed |
420 |
760 |
39 |
Application
Typical Applications of Incoloy 825 include:
- Sulphuric acid piping and vessels
- Phosphoric acid evaporators
- Pickling tank heaters, pickling tanks and equipment
- Chemical process equipment
- Propellor shafts
- Tank trucks
- Calorifiers
- Electrostatic precipitator electrodes
- Hot vessels for food, water and seawater,
- Ammonium sulphate vessels
- Expansion bellows
- Marine exhaust systems
- Power station ash hoppers
Lork Group: Your Trusted Supplier of Incoloy 825 Products
At Lork Group, we specialize in manufacturing and exporting high-quality Incoloy 825 Sheets & Plates tailored to meet stringent industrial requirements. Our products undergo rigorous quality checks to ensure:
Precision engineering for consistent performance.
Strict compliance with international standards (ASTM B424, ASME SB424).
Custom solutions for specific industrial needs.
Whether you need corrosion-resistant sheets for chemical plants or durable plates for offshore oil rigs, we provide reliable, high-performance materials that enhance operational longevity.
Hot Tags: Incoloy 825, Alloy 825, Nickel Sheet, UNS N08825, corrosion-resistant sheet, sulfuric acid resistant, phosphoric acid resistant, pitting-resistant
You Might Also Like
Send Inquiry