CD4MCu is a cast duplex stainless steel with a microstructure consisting of approximately 50% ferrite and 50% austenite. This duplex structure combines the ductility and toughness of austenitic stainless steel with the high strength of ferritic stainless steel, giving it properties far superior to conventional stainless steels.
Size Reference and Applicable Standards
Applicable Standards
ASTM A890
Note: If you have any required standards, please contact us for consultation.
The CD4MCu pipe market is somewhat unique because it is essentially a cast grade. The "pipes" actually in circulation mainly fall into two technical categories, resulting in significant differences in size ranges.
Centrifugally Cast Pipes: This supply method best reflects the inherent properties of CD4MCu material, as it is directly centrifugally cast by the foundry.
Outer Diameter: Typically > 50 mm, falling into the category of large-diameter pipes.
Length: Standard supply lengths are between 1000-2000 mm.
Wall Thickness: Usually customized according to customer drawings
Seamless Pipes:
Outer Diameter Range: 6 mm- 530 mm, covering small to large diameters.
Wall Thickness Range: From thin-walled to thick-walled.
Core Advantages of the Pipe Material
For piping systems, the value of CD4MCu lies in three main aspects:
Resistant to Erosion Corrosion
Its duplex microstructure gives it significantly higher hardness and strength than 316L. In high-speed flow of media containing solid particles (such as slurry, ash, and catalyst particles), the wear rate of the pipe wall is significantly lower than that of conventional austenitic stainless steel.
Resistant to Chloride Pitting/Crevice Corrosion
The synergistic effect of high chromium, molybdenum, copper, and nitrogen allows its critical pitting temperature in neutral or acidic environments containing chloride ions to typically reach above 40°C, making it suitable for seawater, brine, and chlorinated process media.
Design Advantages from High Yield Strength
With a yield strength approximately twice that of 316, theoretically, thinner wall thicknesses can be selected for the same pressure rating, thereby reducing the overall weight of the piping system.
chemical composition
| Element | Range |
| Cr | 24.5 - 26.5 |
| Ni | 4.75 - 6.0 |
| Mo | 1.75 - 2.25 |
| Cu | 2.75 - 3.25 |
| N | CD4MCu: No specification; CD4MCuN: 0.10-0.25 |
| C | ≤ 0.04 |
Important Note: CD4MCu has been removed from some ASTM standards. When purchasing, you should ask the supplier to specify whether the product is CD4MCu or CD4MCuN and verify the nitrogen content.
Physical Properties
| Density | approx. 7.8 g/cm³ |
| Thermal Conductivity | approx. 16.5 W/m·K (100°C) |
| Coefficient of Linear Expansion | approx. 11.5 × 10⁻⁶ /K (20-200°C) |
Mechanical Properties (Pressure Bearing Base for Pipes)
The following are typical minimum values for the solution-treated state:
| Tensile Strength | ≥ 690 MPa |
| Yield Strength | ≥ 485 MPa |
| Elongation | ≥ 16% |
| Hardness | Typical Brinell hardness: approximately 224-295 HBW |
Procurement Considerations
Confirm whether the grade is CD4MCu or CD4MCuN: The original CD4MCu is no longer the current standard.
Confirm the pipe manufacturing process: CD4MCu is a casting grade. If the supplier claims it is "seamless pipe," inquire about the source of the raw materials-is it forged/rolled from ingots, or centrifugally cast billets? Different processes have a significant impact on density and microstructure uniformity.
Request heat treatment records: Request records of solution treatment temperature, holding time, and cooling method.
Verify the PMI (Polymer Spectroscopic Analysis) report: Nitrogen is critical for CD4MCuN, but portable spectrometers (PMIs) typically cannot detect nitrogen. Request the supplier to provide a laboratory chemical analysis report.
Ferrite content testing: Request the supplier to provide a metallographic examination report to confirm that the ferrite content is within the target range. An imbalance in the ferrite ratio will directly lead to a loss of corrosion resistance or toughness.

Pipe Processing and Heat Treatment (Core Challenges)

Solution Treatment
Pipes must undergo solution treatment to achieve a balanced duplex microstructure and optimal corrosion resistance. The solution temperature should not exceed 1120°C; otherwise, ferrite grains will grow abnormally, leading to a sharp decrease in toughness.

Welding
Welding Consumable Selection: Ultra-low carbon duplex steel welding consumables are recommended to ensure the austenite ratio and corrosion resistance of the weld. After welding, pickling and passivation should be performed to restore the corrosion resistance of the weld and heat-affected zone.

Machining and Cold Bending
Cutting: The cutting tool must be sharp, and sufficient coolant must be ensured; otherwise, the surface will work harden, becoming harder with each cut.
Cold Bending: High springback is expected; the die design must allow for allowances.
Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488
Hot Tags: CD4MCu,CD4MCu Pipe,CD-4MCu,UNS J93370,ASTM A890,CD4MCuN Duplex Stainless Steel
You Might Also Like
Send Inquiry