ASTM F2257 / Medical Grade 316LVM Tube

ASTM F2257 / Medical Grade 316LVM Tube

316LVM stainless steel tubing is a medical-grade low-carbon austenitic stainless steel manufactured using vacuum melting technology, resulting in higher cleanliness and reliability. It conforms to ASTM F2257 standards and is available in seamless, welded-drawn, and custom sizes, with options for annealed or cold-worked finishes, as well as custom cutting, grinding, and surface treatment services.
Send Inquiry

Products Description

 

316LVM stainless steel tubing
 
 

316LVM stainless steel tubing is a vacuum-melted low-carbon austenitic stainless steel designed specifically for surgical implants and medical device applications. 316LVM tubing is manufactured according to ASTM F2257 standards and is available in both forged seamless and welded drawn forms. It features excellent corrosion resistance, high cleanliness, good mechanical properties, and reliable biocompatibility. Our company has obtained ISO 9001 and ISO 13485 certifications.

It has a very high application rate in orthopedics and trauma. Typical applications include: Orthopedics and Traumatology: Hip joint stems, femoral heads, bone plates, bone screws, intramedullary nails, spinal systems, knee joint components, etc.

Cardiovascular: Guidewires, cardiac stents.

Other Medical: Dental implants, surgical instruments (such as puncture needles, cannulas), and various temporary fixation devices.

 

Size and price reference

 

This specification applies to cold-finished straight length tubing with a 3 mm [0.125 in.] and smaller nominal outside diameter (OD) and a 0.5 mm [0.020 in.] and thinner nominal wall thickness.

 

High-precision 316LVM tubes are supplied according to ASTM F2257 requirements. Pricing depends on tube dimensions, quantity, surface finish, and certification requirements. Our price range is $150-$200 per kg. The minimum order quantity is 50 kg.

 

Note: Due to the special requirements of implantable-grade orders, including VIM+VAR, full-process traceability, small batches, and high testing requirements, the quoted price is for reference only. Please contact us for more details.

Click to inquire

 

 

Chemical Requirements, Heat Analysis

According to ASTM F2257, the chemical composition should conform to F138 (seamless tube) or F139 (welded and drawn tube). Here, we take seamless tube as an example.

Carbon
0.030 max
Manganese
2.00 max
Phosphorous
0.025 max
Sulfur
0.010 max
Silicon
0.75 max
Chromium
17.00 to 19.00
Nickel
13.00 to 15.00
Molybdenum
2.25 to 3.00
Nitrogen
0.10 max
Copper
0.50 max
Cobalt
<0.10
Iron*
Balance
Composition Index = % Cr + 3.3 × % Mo
26.0 min
* The percentage of iron content by difference is not required to be determined or certified.
Key difference: "L" represents low carbon, and "VM" represents vacuum melting. Compared with ordinary 316L, 316LVM has lower levels of impurities such as carbon, sulfur, and phosphorus, and is of higher purity.

 

Mechanical properties

 

Condition
Wall Thickness, mm [in.]
Ultimate Tensile Strength,
min MPa [psi]
Yield Strength (0.2 % offset),
min MPa [psi]
Elongation (% in 50 mm [2 in.] or 4D),min (%)
Annealed
0.20 [0.008] to 0.46 [0.018] incl
490 [71 000]
190 [27 500]
40
 
0.05 [0.002] to 0.20 [0.008] excl
550 [80 000]
207 [30 000]
35
 
Less than 0.05 [0.002]
586 [85 000]
241 [35 000]
20
 
Cold worked
0.20 [0.008] to 0.46 [0.018] incl
860 [125 000]
690 [100 000]
10
  0.05 [0.002] to 0.20 [0.008] excl
860 [125 000]
690 [100 000]
8
 
Less than 0.05 [0.002]
860 [125 000]
690 [100 000]
4

 

Permissible Variation in OD and ID Dimensions

 

Nominal OD or ID
mm [in.]
Permissible Variation
from Nominal, mm [in.]
Less than 1.5 [0.060]
±0.013 [0.0005]
1.5 to 3.2 [0.060 to 0.125] incl.
±0.025 [0.001]

 

Manufacturing process

 

Surface Finish:

The outer surface of the pipe shall be cold-drawn, bright annealed, ground, or polished.

The maximum outer surface roughness is 0.6 µm [25 µin.] Ra.

 

The inner surface of the pipe shall be cold-drawn or bright annealed.

The maximum inner surface roughness is 0.8 µm [30 µin.] Ra.

The method for determining surface roughness shall be determined through consultation between the buyer and the supplier.

 

Core Characteristics and Performance

 

High Purity from Vacuum Melting

Vacuum arc remelting (VAR) reduces non-metallic inclusions and gas content (such as bubbles).

Adjustable Mechanical Properties

Adjustable through cold working to meet diverse needs.

Excellent Corrosion Resistance

High molybdenum content and high purity resist general corrosion, intergranular corrosion, pitting corrosion, and crevice corrosion.

Good Biocompatibility

Its surface oxide layer is relatively stable, causing minimal tissue reactions in vivo.

 

Limitations and Precautions

 

Ni nickel ion release: During long-term implantation, nickel ions may be slowly released, posing a potential risk of sensitization or toxicity. This is a focus of ongoing research in materials science.

Imaging artifacts: Compared to titanium alloys, 316LVM produces more noticeable artifacts on MRI scans, potentially affecting postoperative imaging assessment.

Corrosion risk: Despite its excellent corrosion resistance, crevice corrosion can still occur in hypoxic environments such as at joints between multiple implant components (e.g., the interface between screws and bone plates).

Imaging artifacts

 

 

 Lork Group
 Marketing Operations Department
 Email: layla@lorkgroup.com
 WhatsApp: +86 199 3707 5488

Hot Tags: 316LVM Tube,316LVM Stainless Steel Tube, Medical Grade 316LVM Tube,ASTM F2257,316LVM Seamless Tube,Surgical Instrument Tubing,Implant Grade Stainless Steel Tubing

Send Inquiry