UNS N06002 / Hastelloy X Tube
Hastelloy X Tube is a high temperature and corrosion resistant nickel-based solid solution strengthened alloy. This alloy has outstanding resistance to oxidation and possesses exceptional strength at elevated temperatures. It has high strength up to 1500ºF (816ºC) and good oxidation resistance up to 2200ºF (1204ºC).
Lork Group offer comprehensive solutions including plate, sheet, strip, billet, bar, wire, pipe & tubing. Hastelloy X Tube is used extensively in high temperature jet engine and chemical processing applications and is highly resistant to stress corrosion cracking in petrochemical applications. Request your free quote and technical data today!
UNS N06002 Hastelloy X Tube Specifications
| Size | 15 NB to 150 NB IN |
| Type | Seamless / ERW / Welded / Fabricated / Hollow / LSAW Pipes |
| wall thickness | .035" –.095′, (special wall thicknesses available) |
| Schedule | SCH5, SCH10, SCH40, STD, SCH80, SCH160 |
| Finish | Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF |
| Form | Round, Square, Rectangular, Hydraulic, Straight or 'U' bent Tubes Etc. |
| Length | Single Random, Double Random & Cut Length. |
| End | Plain End, Beveled End, Treaded |
Chemical Composition
| Element | Content (%) |
|---|---|
| Cr, Chromium | 20.5-23 |
| Fe, Iron | 17-20 |
| Mo, Molybdenum | 8-10 |
| Mn, Manganese | 1 max |
| Si, Silicon | 1 max |
| Ti, Titanium | 0.15 max |
| Co, Cobalt | 0.5-2.5 |
| Al, Aluminum | 0.5 max |
| Cu, Copper | 0.5 max |
| C, Carbon | 0.05-0.15 |
| P, Phosphorus | 0.04 max |
| S, Sulfur | 0.03 max |
| W, Tungsten | 0.2-1 |
| B, Boron | 0.008 max |
| Ni, Nickel | Remainder |
Alloy X Tube Mechanical Properties
| Properties | Metric | Imperial |
|---|---|---|
| Tensile strength (@ 1093°C/1999°F, thickness 1.10-1.60 mm/0.0433-0.0630 in.) | 110 MPa | 16000 psi |
| Yield strength (@ 1093°C/1999°F, thickness 1.10-1.60 mm/0.0433-0.0630 in., 0.2% offset) | 52 MPa | 7540 psi |
| Elastic modulus | 212 GPa | 30700 ksi |
| Elongation at break (@ 982°C/1800°F, thickness 1.10-1.60 mm/0.0433-0.0630 in., in 50.8 mm) | 46% | 46% |
| Charpy Impact (V Notch; solution heat-treated, not aged) | 190 J | 140 ft-lb |
Applications of Hastelloy X tubing include
- Gas Turbine Components
- Aerospace Industry: exhaust systems, afterburners, and structural components
- Industrial Furnaces
- Chemical Processing
- radiant tubes, muffles, and heat exchangers
For applications demanding exceptional strength and oxidation resistance in extreme temperature environments, Hastelloy X stands as the material of choice among engineering alloys. Lork Group is a leading global exporter of high-performance nickel alloys, specializing in comprehensive Hastelloy X product solutions for the world's most demanding industrial applications. We deliver material excellence and reliable global supply chain support for your most critical projects.
Contact Lork Group today to discuss your project requirements, receive a competitive international quotation, and arrange for your free sample. Discover why we are the trusted choice for high-performance alloy solutions worldwide.