AMS 5590 Inconel 718 Tubing(UNS N07718)

AMS 5590 Inconel 718 Tubing(UNS N07718)

AMS 5590 Inconel 718 tubing (UNS N07718) is a nickel-based precipitation-hardening superalloy manufactured using controlled melting processes, including vacuum melting, to ensure its chemical composition and metallurgical quality. This tubing is supplied in seamless form and is suitable for aerospace fluid systems, aircraft engine components, and other high-performance applications.
Send Inquiry

Products Description

 

AMS 5590 Inconel 718 tubing is a nickel-chromium-iron-based superalloy seamless tube designed for applications requiring high mechanical strength, corrosion resistance, and reliable performance in both high- and low-temperature environments.

 

This material is produced using a consumable electrode or vacuum induction melting and is solution-treated at 1066°C (1950°F). It is particularly suitable for fluid piping and structural components that may require forming or welding followed by heat treatment.

 

Size information

 

This specification covers a corrosion- and heat-resistant nickel alloy in the form of seamless tubing having a nominal OD of 0.125 inch (3.18 mm) and over with a nominal wall thickness of 0.015 inch (0.38 mm) and over.

Contact now

 

 

chemical composition

 

Element %
Iron remainder
Copper
0.30
Boron
0.006
Tantalum
0.05
Cobalt
1.00
Aluminum
0.20-0.80
Titanium
0.65-1.15
Columbium (Niobium)
4.75-5.50
Molybdenum
2.80-3.30
Nickel
50.5-54.5
Chromium
17.0-21.0
Sulfur
0.015
Phosphorus
0.015
Silicon
0.35
Manganese
0.35
Carbon
0.08

*This component was determined according to the ASTM E354 standard.

 

Tensile Properties

 

For pipes with a nominal outer diameter of 0.125 inches (3.18 mm) and above and a nominal wall thickness of 0.015 inches (0.38 mm) and above, this performance is determined according to ASTM E8/E8M standards.

 

As Solution Heat Treated
After Precipitation Heat Treatment
Tensile Strength, max
145 ksi (1000 MPa)
Tensile Strength, min
170 ksi (1172 MPa)
Yield Strength at 0.2% Offset, max
85 ksi ( 586 MPa)
Yield Strength at 0.2% Offset, min
145 ksi (1000 MPa)
Elongation in 2 Inches (50.8 mm), min
30%
Elongation in 2 Inches (50.8 mm), min
15%

 

Manufacturing Process

Manufacturing AMS 5590 Inconel 718 Tubing (UNS N07718) involves controlled melting, seamless tube forming, cold drawing, and solution heat treatment. Each stage is carefully controlled to ensure chemical composition, dimensional accuracy, and consistent material quality for aerospace applications.

Vacuum melting furnace

1. Melting & Alloy Preparation: Selected raw materials are melted under controlled conditions to achieve the required chemical composition and metallurgical quality.

2. Billet Preparation & Hot Working: Alloy billets are heated and processed through hot extrusion or piercing to produce seamless hollow tubes.

3. Cold Drawing: Tubes are drawn through precision dies to control outside diameter, wall thickness, dimensional tolerances, and surface finish. Intermediate annealing may be applied when necessary.

4. Solution Heat Treatment: Tubing is solution heat-treated at approximately 1950°F (1066°C) according to AMS 5590 requirements to establish the specified metallurgical condition.

5. Finishing & Inspection: Final operations include straightening, cutting, surface finishing, and dimensional inspection. Chemical analysis, mechanical testing, and nondestructive testing are performed as required.

Solution heat treatment

 

Grain Size

 

Grain Size: The average grain size of AMS 5590 Inconel 718 Tubing shall be ASTM No. 3 or finer, as determined in accordance with ASTM E112.

Note: Testing is performed after solution heat treatment; samples are taken from the finished tube.

 

Flarability

 

AMS 5590 specifies flaring requirements for tubing with nominal outside diameters ranging from 0.188 to 2.000 inches (4.78–50.80 mm), inclusive.

At room temperature, specimens must withstand the flaring test without developing cracks or other visible defects. The test is performed by forcing the tubing axially over a hardened and polished tapered steel pin with a 74° included angle.

The permanent expanded outside diameter must reach at least 1.25 times the original nominal outside diameter.

Flaring Test

 

FAQ

 

Q: What is the difference between AMS 5590 and AMS 5589?

A: Both specifications cover Inconel 718 seamless tubing, but they differ in their specified solution heat-treatment temperatures. AMS 5590 specifies 1950°F (1066°C), while AMS 5589 specifies 1775°F (968°C). Buyers should select the specification according to their engineering requirements.

Q: Is AMS 5590 Inconel 718 tubing seamless or welded?

A: AMS 5590 covers seamless Inconel 718 tubing. It is manufactured through processes such as hot working and subsequent cold drawing to achieve the required dimensions and surface quality.

Q: How is AMS 5590 Inconel 718 tubing packaged for shipment?

A: Tubing is packaged according to commercial shipping practices and applicable transportation regulations. Protective wrapping, end caps, and secure bundling may be used to prevent surface damage, contamination, and deformation during transportation.

Q: What inspection documents are available?

A: Depending on the order requirements, documentation may include:
The pipe manufacturer shall provide a report with each shipment stating the manufacturer's name and the country of metal melting (e.g., final melting if the metal is processed through multiple melting operations), as well as the composition of each heat, tensile properties and average grain size of each batch, test results for solution heat treatment and precipitation heat treatment for tensile properties, and a statement indicating that the product meets other technical requirements. The report shall include the purchase order number, heat number, batch number, AMS5590G, dimensions, and quantity.

 

Lork Group
Marketing Operations Department
Email: layla@lorkgroup.com
WhatsApp: +86 199 3707 5488

Hot Tags: AMS 5590 Inconel 718 Tubing, Inconel 718 Seamless Tubing, UNS N07718, Aerospace Tubing, Nickel Alloy 718 Tube, Vacuum Melted Tubing, High Strength Nickel Alloy Tubing, aerospace

Send Inquiry