AISI 310 Stainless Steel Bar (UNS S31000)
Lork Group as a professional trustworthy Stainless Steel supplier and exporter, we produce AISI 310 bars & rods with high cost performance.
AISI 310 bars are a type of stainless steel known for high heat and corrosion resistance. Composed of 24% chromium, 19% nickel, and 6% manganese. They are popular in various industries, such as petrochemical, pharmaceutical, and chemical processing.
AISI 310 bar is an austenitic stainless steel grade. The Stainless Steel 310 Round Bar is designed with a chemical content of chromium, carbon, manganese, nickel, phosphorous, sulfur, silicon, and iron. 310 Stainless Steel Round Bar is produced with a circular cross sectional area and exhibits superior resistance to corrosive and oxidative media across stress-induced setups.
AISI 310 bar is utilized across high temperatures up to 1150 degrees C. These components perform well in carburizing environments and show enhanced toughness. The AISI 310S Polished Bar is an aesthetically appealing grade that is manufactured possessing different types of surface finishes. These bars are customizable in different shapes and sizes to meet all customer requirements.
The ASTM A276 type 310 Hex Bar is a unique bar having 6 sides. The geometry of these bars allows them to be moved and rotated with ease in the system. AMS 5521 Hex Bar is dimensionally accurate and is widely seen in chemical equipment, aerospace, marine, and other industries.
AISI 310 Bar is designed possessing a square cross-sectional area. These bars are common features in packing and manufacturing units. The 310 Stainless Steel Flat Bar is designed with a rectangular cross-section. The bars have lower thickness than square bars and are lightweight. ASTM A276 UNS S31008 Rectangle Bar is a non-pressurized module that is designed for applications that don't usually require items having precise sizes and tolerance. These bars are produced making use of the latest technology and the best raw materials.
As a leading AISI 310 Stainless Steel supplier in China, our products pass strict quality control and testing and ensure that the products meet standards and customer requirements. Lork Group manufactures and produces AISI 310 Bar of various sizes.
Specification
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Hex Bars in Milimeter |
18mm – 57mm (11/16″ to 2-3/4″) |
|
Round Bars Diameter |
Outside Diameter in the range of 4mm to 500mm |
|
Bright Bars Diameter |
Outside Diameter in the range of 4mm to 100mm |
|
Square Bars in Milimeter |
18mm – 47mm (11/16″ to 1-3/4″) |
|
Finish |
Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
|
Length |
1 to 6 Meters, Custom Cut Lengths |
|
Flat Bars in Milimeter |
1/2" to 10" in thickness range of 2mm to 150mm, |
|
Form |
Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
Chemical Composition
|
Element |
Weight% |
|
C |
0.015 max |
|
Mn |
2.0 max |
|
Si |
0.15 max |
|
P |
0.020 max |
|
S |
0.015 max |
|
Cr |
24.00 - 26.00 |
|
Ni |
19.00 - 21.00 |
|
Mo |
0.10 max |
|
N |
54.7 min |
Mechanical Properties
|
Density |
7.9 g/cm³ |
|
Melting Point |
1402 °C (2555 °F) |
|
Tensile Strength |
Psi – 75000 , MPa – 515 |
|
Yield Strength (0.2%Offset) |
Psi – 30000 , MPa – 205 |
|
Elongation |
40 % |
Hot Forming and Cold Forming of AISI 310 Flat Bar
Hot Forming
Heat to a consistent temperature of 1742–2192°F (950–1200°C). A final anneal at 1832 – 2101°F (1000 – 1150°C) followed by quick quenching is advised after hot forming.
Cold Forming
The alloy is ductile and forms in a similar way to 316 stainless steel. Because the alloy is susceptible to carbide precipitation and sigma phase precipitants, cold forming of components with long-term exposure to high temperatures is not suggested.
Applications
- Oil and Gas Industries
- Food Processing Industries
- Equipments
- Pipeline
- Power Industries
- Ship Building Industries
- Paper Industries
- Cement Industries
- Chemical Industries
- Railways
- Electric Motors & Pumps
- Agriculture
- Automobiles
- Hoses & Fittings
- Mining
- Shaft Making
- Miscellaneous Fabrication Jobs
- Tools & Fixtures (including strapping, banding, buckles & brackets)
- Ornamental Iron Work
- Manufacturing Parts & Equipment
- Machinery Frames