AISI 304L Stainless Steel Bar (UNS S30403)
Lork Group, as a professional, trustworthy Stainless Steel supplier and exporter, we produce AISI 304L bars & rods with high cost performance.
Stainless steel 304L is a low-carbon version of 304 and is used in welding applications. It has the same properties as 304 but is less likely to sensitize during welding, making it a popular choice in applications where welding is required. It is also commonly used in the food and beverage industry and architectural and chemical applications.
AISI 304L bar is the standard "18/8" stainless; it is the most versatile and most widely used stainless steel, available in a wider range of products, forms and finishes than any other. It has excellent forming and welding characteristics. The balanced austenitic structure of Grade 304l enables it to be severely deep drawn without intermediate annealing, which has made this grade dominant in the manufacture of drawn stainless parts such as sinks, hollow-ware and saucepans. For these applications it is common to use special "304lDDQ" (Deep Drawing Quality) variants.
As a leading AISI 304L Stainless Steel supplier in China, our products pass strict quality control and testing and ensure that the products meet standards and customer requirements. Lork Group manufactures and produces AISI 304L bars of various sizes.
Specification
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Hex Bars in Milimeter |
18mm – 57mm (11/16″ to 2-3/4″) |
|
Round Bars Diameter |
Outside Diameter in the range of 4mm to 500mm |
|
Bright Bars Diameter |
Outside Diameter in the range of 4mm to 100mm |
|
Square Bars in Milimeter |
18mm – 47mm (11/16″ to 1-3/4″) |
|
Finish |
Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish |
|
Length |
1 to 6 Meters, Custom Cut Lengths |
|
Flat Bars in Milimeter |
1/2" to 10" in thickness range of 2mm to 150mm, |
|
Form |
Round, Square, Hex (A/F), Rectangle, Billet, Ingot, Forging Etc. |
|
Dimensions |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
Chemical Composition
|
Element |
Weight% |
|
C |
0.035 max |
|
Mn |
2.0 max |
|
Si |
1.0 max |
|
P |
0.045 max |
|
S |
0.030 max |
|
Cr |
18.0 - 20.0 |
|
Ni |
8-13 |
|
Mo |
- |
Mechanical Properties
|
Density |
8.0 g/cm³ |
|
Melting Point |
1400 °C (2550 °F) |
|
Tensile Strength |
Psi – 75000 , MPa – 515 |
|
Yield Strength (0.2%Offset) |
Psi – 30000 , MPa – 205 |
|
Elongation |
35 % |
Applications
AISI 304L bar is ideal for both commercial and at-home applications. Some specific examples of uses for this grade of steel can include:
- Aerospace and automotive structures
- Architectural paneling, molding, trim and other details
- Braces
- Chemical containers to be used for transport
- Cooking tools (such as pots and pans)
- Construction material for buildings
- Dyeing
- Food processing equipment (such as wine, beer brewing, and milk)
- Heat exchangers
- Kitchen equipment (such as sinks or appliances)
- Marine environment equipment (such as nuts, screws or bolts)
- Railing and trim
- Springs
- Threaded fasteners
- Welded or woven water filtration screens
Due to its immense versatility, 304L can be used across a wide variety of industrial applications, especially in high-corrosion environments.
Hot Tags: 304L Stainless Steel Bar, AISI 304L, UNS S30403, low-carbon stainless bar, weldable stainless bar, corrosion-resistant bar, austenitic stainless round bar
You Might Also Like
Send Inquiry